| 液-固电迁移Ni/Sn-9Zn/Ni焊点反极性效应研究 |
黄明亮( ), 张志杰, 冯晓飞, 赵宁 |
| 大连理工大学材料科学与工程学院, 大连 116024 |
|
| REVERSE POLARITY EFFECT IN Ni/Sn-9Zn/Ni INTERCONNECT UNDERGOING LIQUID- SOLID ELECTROMIGRATION |
HUANG Mingliang( ), ZHANG Zhijie, FENG Xiaofei, ZHAO Ning |
| School of Materials Science & Engineering, Dalian University of Technology, Dalian 116024 |
引用本文:
黄明亮, 张志杰, 冯晓飞, 赵宁. 液-固电迁移Ni/Sn-9Zn/Ni焊点反极性效应研究[J]. 金属学报, 2015, 51(1): 93-99.
Mingliang HUANG,
Zhijie ZHANG,
Xiaofei FENG,
Ning ZHAO.
REVERSE POLARITY EFFECT IN Ni/Sn-9Zn/Ni INTERCONNECT UNDERGOING LIQUID- SOLID ELECTROMIGRATION[J]. Acta Metall Sin, 2015, 51(1): 93-99.
| [1] |
Hsiao H Y, Liu C M, Lin H W, Liu T C, Lu C L, Huang Y S, Chen C, Tu K N. Science, 2012; 336: 1007
|
| [2] |
Huang M L, Zhou S M, Chen L D. J Electron Mater, 2012; 41: 730
|
| [3] |
Chen C, Tong H M, Tu K N. Annu Rev Mater Res, 2010; 40: 531
|
| [4] |
Huang M L, Ye S, Zhao N. J Mater Res, 2012; 26: 3009
|
| [5] |
Blech I A, Meieran E S. Appl Phys Lett, 1967; 11: 263
|
| [6] |
Chen S W, Chen C M, Liu W C. J Electron Mater, 1998; 27: 1193
|
| [7] |
Chen C M, Chen S W. J Electron Mater, 1999; 28: 902.
|
| [8] |
Gan H, Tu K N. In: Scott N ed., Proceedings IEEE 52nd Electronic Components and Technology Conference (ECTC 2002), San Diego: IEEE, 2002: 1206
|
| [9] |
Zhang X F, Guo J D, Shang J K. Scr Mater, 2007; 57: 513
|
| [10] |
Zhang X F, Guo J D, Shang J K. J Mater Res, 2008; 23: 3370
|
| [11] |
Huang M L, Zhou Q, Zhao N, Liu X Y. J Mater Sci, 2014; 49: 1755
|
| [12] |
Huang M L, Zhou Q, Zhao N, Zhang Z J. J Electron Mater, 2013; 42: 2975
|
| [13] |
Huang M L, Zhang Z J, Zhao N, Zhou Q. Scr Mater, 2013; 68: 853
|
| [14] |
Huang M L, Zhang Z J, Zhao N, Yang F. J Alloys Compd, 2014; doi: 10.1016/j.jallcom.2014.08.263
|
| [15] |
Liou W K, Yen Y W, Jao C C. J Electron Mater, 2009; 38: 2222
|
| [16] |
Wang C H, Chen H H. J Electron Mater, 2010; 39: 2375
|
| [17] |
Huntington H B, Grone A R. J Phys Chem Solids, 1961; 20: 76
|
| [18] |
Ho P S, Kwok T. Rep Prog Phys, 1989; 52: 301
|
| [19] |
Blech I A. J Appl Phys, 1976; 47: 1203
|
| [20] |
Tu K N. Phys Rev, 1992; 45B: 1409
|
| [21] |
Smolin M D, Frantsevich I N. Sov Phys-Sol, 1962; 3: 1536
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|