| 304不锈钢毛细管/Zr53.5Cu26.5Ni5Al12Ag3块体非晶合金复合材料的制备与性能研究 |
马广财1, 付华萌1, 王峥2, 徐庆亮3, 张海峰1( ) |
1 中国科学院金属研究所沈阳材料科学国家(联合)实验室, 沈阳110016 2 沈阳科金新材料有限公司, 沈阳110016 3 中国石油大庆石化分公司腈纶厂, 大庆 163714 |
|
| STUDY ON FABRICATION AND PROPERTIES OF 304 STAINLESS STEEL CAPILLARY TUBES/Zr53.5Cu26.5Ni5Al12Ag3 BULK METALLIC GLASS COMPOSITES |
MA Guangcai1, FU Huameng1, WANG Zheng2, XU Qingliang3, ZHANG Haifeng1( ) |
1 Shenyang National Laboratory for Materials Science, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016 2 Shenyang Kejin Advanced Material Company Limited, Shenyang 110016 3 Petrochina Daqing Petrochemical Company Acrylic Fiber Plant, Daqing 163714 |
引用本文:
马广财, 付华萌, 王峥, 徐庆亮, 张海峰. 304不锈钢毛细管/Zr53.5Cu26.5Ni5Al12Ag3块体非晶合金复合材料的制备与性能研究[J]. 金属学报, 2014, 50(9): 1087-1094.
Guangcai MA,
Huameng FU,
Zheng WANG,
Qingliang XU,
Haifeng ZHANG.
STUDY ON FABRICATION AND PROPERTIES OF 304 STAINLESS STEEL CAPILLARY TUBES/Zr53.5Cu26.5Ni5Al12Ag3 BULK METALLIC GLASS COMPOSITES[J]. Acta Metall Sin, 2014, 50(9): 1087-1094.
| [1] |
Ashby M F, Greer A L. Scr Mater, 2006; 54: 3216
|
| [2] |
Gilbert C T, Ritchie R O, Johnson W L. Appl Phys Lett, 1997; 71: 476
|
| [3] |
Suzuki K, Kataoka N, Inoue A. Mater Trans JIM, 1990; 31: 743
|
| [4] |
Inoue A, Zhang T, Masumoto T. Mater Trans JIM, 1995; 36: 391
|
| [5] |
Deng S T, Zhang H F, Wang A M, Li H, Ding B Z, Hu Z Q. J Alloys Compd, 2008; 406: 182
|
| [6] |
Inoue A, Takeuchi A. Acta Mater, 2011; 59: 2243
|
| [7] |
Lottler J. Intermetallics, 2003; 11: 529
|
| [8] |
Szuecs F, Kim C P, Johnson W L. Acta Mater, 2001; 49: 1507
|
| [9] |
Zhang B, Zhao D Q, Pan M X. Phys Rev Lett, 2005; 94: 205502
|
| [10] |
Johnson W L. Appl Phys Lett, 1999; 24: 42
|
| [11] |
Zhu Z W. PhD Dissertation, Institute of Metal Research, Chinese Academy of Sciences, Shenyang, 2009
|
| [11] |
(朱正旺. 中国科学院金属研究所博士学位论文, 沈阳, 2009)
|
| [12] |
Zhu Z W, Zhang H F, Hu Z Q, Zhang W, Inoue A. Scr Mater, 2010; 62: 278
|
| [13] |
Kuhn U, Eckert J, Mattern N, Schultz L. Appl Phys Lett, 2002; 80: 2478
|
| [14] |
Fan C, Ott R T, Hufnagel T C. Appl Phys Lett, 2002; 81: 1020
|
| [15] |
Bian Z, Kato H, Qin C, Zhang W, Inoue A. Acta Mater, 2005; 53: 2037
|
| [16] |
Dong W B, Zhang H F, Sun W S, Wang A M, Li H, Hu Z Q. J Mater Res, 2006; 21: 1490
|
| [17] |
Hui X, Dong W, Chen G L. Acta Mater, 2007; 55: 907
|
| [18] |
Hofmann D C, Suh J Y, Wiest A. Nature, 2008; 451: 1085
|
| [19] |
Dandliker R B. PhD Dissertation, California Institute of Technology, Pasadena, 1998
|
| [20] |
Fan C, Li L, Kelskes J, Liu C T. Phys Rev Lett, 2006; 96: 145506
|
| [21] |
Kim C P. PhD Dissertation, California Institute of Technology, Pasadena, 2001
|
| [22] |
Conner R D. PhD Dissertation, California Institute of Technology, Pasadena, 1998
|
| [23] |
Lee S Y. PhD Dissertation, California Institute of Technology, Pasadena, 2007
|
| [24] |
Mathaudhu S N. PhD Dissertation, Texas A&M University, College station, 2006
|
| [25] |
Wang G. PhD Dissertation, The University of Tennessee, Knoxiville, 2006
|
| [26] |
Hofmann D C. PhD Dissertation, California Institute of Technology, Pasadena, 2009
|
| [27] |
Chen L Y, Fu Z D, Zhang G Q, Hao X P, Jiang Q K, Wang X D, Cao Q P. Phys Rev Lett, 2008; 100: 075501
|
| [28] |
Deng S T, Diao H, Chen Y L. Scr Mater, 2011; 64: 85
|
| [29] |
Deng S T. PhD Dissertation, Institute of Metal Research, Chinese Academy of Sciences, Shenyang, 2010
|
| [29] |
(邓胜涛. 中国科学院金属研究所博士学位论文, 沈阳, 2010)
|
| [30] |
Sun Y, PhD Dissertation, Institute of Metal Research, Chinese Academy of Sciences, Shenyang, 2010
|
| [30] |
(孙 羽. 中国科学院金属研究所博士学位论文, 沈阳, 2010)
|
| [31] |
Zheng Q, Cheng S, Strader J H, Ma E, Xu J. Scr Mater, 2007; 56: 161
|
| [32] |
Park E S, Lee J Y, Kim D H, Gebert A, Schultz L. J Appl Phys, 2008; 104: 023520
|
| [33] |
Lee C J, Huang J C, Nieh T G. Appl Phys Lett, 2007; 91: 161963
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|