| 多晶Be室温拉伸变形和断裂行为 |
许德美1,2, 秦高梧1( ), 李峰2, 王战宏2, 钟景明2, 李志年2, 何力军3 |
1 东北大学材料各向异性与织构教育部重点试验室, 沈阳110819 2 西北稀有金属材料研究院宁夏特种材料重点实验室, 石嘴山753000 3 宁夏大学宁夏光伏材料重点实验室, 银川750021 |
|
| TENSILE DEFORMATION AND FRACTURE BEHAVIOR OF POLYCRYSTALLINE BERYLLIUM AT ROOM TEMPERATURE |
XU Demei1,2, QIN Gaowu1( ), LI Feng2, WANG Zhanhong2, ZHONG Jingming2, LI Zhinian2, HE Lijun3 |
1 Key Laboratory for Anisotropy and Texture of Materials (Ministry of Education), Northeastern University, Shenyang 110819 2 Key Laboratory of Ningxia for Rare Materials, Northwest Rare Metal Materials Research Institute, Shizuishan 753000 3 Key Laboratory of Ningxia for Photovoltaic Materials, Ningxia University, Yinchuan 750021 |
引用本文:
许德美, 秦高梧, 李峰, 王战宏, 钟景明, 李志年, 何力军. 多晶Be室温拉伸变形和断裂行为[J]. 金属学报, 2014, 50(9): 1078-1086.
Demei XU,
Gaowu QIN,
Feng LI,
Zhanhong WANG,
Jingming ZHONG,
Zhinian LI,
Lijun HE.
TENSILE DEFORMATION AND FRACTURE BEHAVIOR OF POLYCRYSTALLINE BERYLLIUM AT ROOM TEMPERATURE[J]. Acta Metall Sin, 2014, 50(9): 1078-1086.
| [1] |
Goldberg A. Atomic, Crystal, Elastic, Thermal, Nuclear and Other Properties of Beryllium. Livermore: Lawrence Livermore National Laboratory, 2006: 3
|
| [2] |
Goldberg A, Olson D L, Jacobson L A. In: Walsh K A ed., Beryllium Chemistry and Processing. Materials Park, OH: The Materials Information Society/ASM International, 2009: 151
|
| [3] |
Marder J M. In: ASM International ed., Metals Handbook: Powder Metallurgy. Vol.7, 9th Ed., Materials Park, OH: American Society for Metals, 1984: 755
|
| [4] |
Webster D. In: The Metals Society ed., Berylllium 1977—Fourth International Conference on Beryllium, London: The Royal Society, 1977: 1/1
|
| [5] |
Fritz A. In: Webster D, London G J eds., Beryllium Science and Technology. Vol.1, New York and London: Plenum Press, 1979: 7
|
| [6] |
Saxton H J,London G J. In: Webster D, London G J eds., Beryllium Science and Technology. Vol.1, New York and London: Plenum Press, 1979: 115
|
| [7] |
Lemon D D, Brown W F. J Test Eval, 1985; 13: 152
|
| [8] |
Burns S J, Gurland J, Richman M H. Metallography, 1971; 4: 533
|
| [9] |
Cooper R E. J Test Eval, 1975; 3: 87
|
| [10] |
Cooper R E. Int J Fract, 1975; 11: 649
|
| [11] |
Conrad H, Hurd J, Woodard D. J Test Eval, 1973; 1: 88
|
| [12] |
Jones M H, Bubsey R T, Brown W F. J Test Eval, 1973; 1: 100
|
| [13] |
Shabbits W O, Logsdon W A. J Test Eval, 1973; 1: 110
|
| [14] |
Kornienko L A, Papirov I I. Met Sci Heat Treat, 1970; 12: 885
|
| [15] |
Perra M W, Finnie I. J Mater Sci, 1977; 12: 1519
|
| [16] |
Bat'kov Yu V, Golubev V K, Sobolev Yu S, Trunin I R, Fishman N D. J Appl Mech Tech Phys, 1996; 37: 484
|
| [17] |
Chaouadi R, Moons F, Puzzolante J L.Tensile and Fracture Toughness Test Results of Neutron Irradiated Beryllium. Tokyo: Japan Atomic Energy Research Institute, 1998: 1
|
| [18] |
Moons F, Chaouadi R, Puzzolante J L. Fusion Eng Des, 1998; 41: 187
|
| [19] |
Taylor G I. J Inst Met, 1938; 62: 307.
|
| [20] |
von Mises R, Angew Z. Math Mech, 1928; 8: 161.
|
| [21] |
Tuer G L, Kaufmann A R. In: White D W, Burke J E eds., The Metal Beryllium. Cleveland: American Society for Metals, 1955: 372
|
| [22] |
Greetham G, Martin A J. In: Institute of Metals ed., The Metallurgy of Beryllium. London: Chapman & Hall Ltd, 1963: 47
|
| [23] |
Martin A J, Ellis G C. In: Institute of Metals ed., The Metallurgy of Beryllium. London: Chapman & Hall Ltd, 1963: 3
|
| [24] |
Bennett W D. In: Institute of Metals ed., The Metallurgy of Beryllium. London: Chapman & Hall. Ltd, 1963: 33
|
| [25] |
Greenspan J. In: Hausner H H ed., Beryllium: its Metallurgy and Properties. Berkeley and Los Angeles: University of California Press, 1965: 240
|
| [26] |
Gindin I A, Grinyuk V N, Ivanov V Y, Lazareva M B, Papirov I I, Starodubov Y D, Tikhinskiy G F, Finkel V A. Phys Met Metall, 1968; 26: 152
|
| [27] |
Yoo M H. Metall Trans, 1981; 12A: 409
|
| [28] |
Liang N G, Liu H Q, Wang Z Q. Sci China, 1995; 25A: 859
|
| [28] |
(梁乃刚, 刘洪秋, 王自强. 中国科学, 1995; 25A: 859)
|
| [29] |
Xu B A,Li X Z. Mechanics of Materials. Shanghai: Shanghai Jiao Tong University Press, 1988: 28
|
| [29] |
(许本安,李秀治. 材料力学. 上海: 上海交通大学出版社, 1988: 28)
|
| [30] |
Shi D K. Fundamentals of Materials Science. 2nd Ed., Beijing: China Machine Press, 2003: 334
|
| [30] |
(石德珂.材料科学基础. 第二版, 北京: 机械工业出版社, 2003: 334)
|
| [31] |
Ha K F. Microscopic Theory of the Metals Mechanical Properties. Beijing: Science Press,1983: 305, 610-615
|
| [31] |
(哈宽富.金属力学性质的微观理论. 北京: 科学出版社, 1983: 305, 610-615)
|
| [32] |
Stroh A N. Proc Math Phys Sci, 1954; 223: 404
|
| [33] |
Stroh A N. Proc Math Phys Sci, 1955; 232: 548
|
| [34] |
Stroh A N. Philos Mag, 1958; 3: 625
|
| [35] |
Xu D M, Li F, Wang D X, Ren Y P, Pei W L, Qin G W. China J Rare Met, 2010; 34: 844
|
| [35] |
(许德美, 李 峰, 王东新, 任玉平, 裴文利, 秦高梧. 稀有金属, 2010; 34: 844)
|
| [36] |
Stonehouse A J. J Vac Sci Technol, 1986; 4A: 1163
|
| [37] |
Matysina Z A. Mater Chem Phys, 1999; 60: 70
|
| [38] |
Gilman J J. Trans Am Inst Min Metall Eng, 1956; 206: 1326
|
| [39] |
Wang L,Lv J Y,Guan F A. Metal Mechanical Property. 5th Ed., Shenyang: Northeastern University Press, 1993: 145
|
| [39] |
(王 磊,吕俊英,关福安. 金属力学性质. 第五版. 沈阳: 东北大学出版社, 1993: 145)
|
| [40] |
Li J. Fundamentals of Materials Science. Beijing: Metallurgical Industry Press, 2006: 216
|
| [40] |
(李见.材料科学基础. 北京: 冶金工业出版社, 2006: 216)
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|