定向凝固Ti-52%Al合金热稳定处理及其对微观组织的影响* |
刘国怀, 张元, 李新中( ), 陈瑞润, 苏彦庆, 郭景杰, 傅恒志 |
哈尔滨工业大学材料科学与工程学院, 哈尔滨 150001 |
|
THERMAL STABILIZATION TREATMENT AND THE EFFECT ON THE MICROSTRUCTURE IN DIRECTIONALLY SOLIDIFIED Ti-52%Al ALLOY |
LIU Guohuai, ZHANG Yuan, LI Xinzhong( ), CHEN Ruirun, SU Yanqing, GUO Jingjie, FU Hengzhi |
School of Materials Science and Engineering, Harbin Institute of Technology, Harbin 150001 |
引用本文:
刘国怀, 张元, 李新中, 陈瑞润, 苏彦庆, 郭景杰, 傅恒志. 定向凝固Ti-52%Al合金热稳定处理及其对微观组织的影响*[J]. 金属学报, 2014, 50(3): 329-336.
Guohuai LIU,
Yuan ZHANG,
Xinzhong LI,
Ruirun CHEN,
Yanqing SU,
Jingjie GUO,
Hengzhi FU.
THERMAL STABILIZATION TREATMENT AND THE EFFECT ON THE MICROSTRUCTURE IN DIRECTIONALLY SOLIDIFIED Ti-52%Al ALLOY[J]. Acta Metall Sin, 2014, 50(3): 329-336.
[1] |
Mullins C W, Sekerka R F. Appl Phys, 1964; 35: 444
|
[2] |
Geng X G, Cheng G, Fu H Z. Acta Metall Sin, 2002; 38: 225
|
[2] |
(耿兴国, 陈 光, 傅恒志. 金属学报, 2002; 38: 225)
|
[3] |
Bosenberg U, Buchmann M, Rettenmayr M. J Cryst Growth, 2007; 304: 281
|
[4] |
Thi H N, Drevet B, Debierre J M. J Cryst Growth, 2003; 253: 539
|
[5] |
Buchmann M, Rettenmayr M. J Cryst Growth, 2005; 284: 544
|
[6] |
Su Y Q, Liu D M, Li X Z, Luo L S, Guo J J, Fu H Z. J Cryst Growth, 2010; 312: 2441
|
[7] |
Umeda T, Okane T, Kurz W. Acta Mater, 1996; 44: 4209
|
[8] |
Trivedi R, Park J S. J Cryst Growth, 2002; 235: 572
|
[9] |
Lo T S, Dobler S, Plapp M, Karma A, Kurz W. Acta Mater, 2003; 51: 599
|
[10] |
Asta M, Beckman C, Karma A. Acta Mater, 2009; 57: 941
|
[11] |
Liu G H, Li X Z, Su Y Q, Liu D M, Guo J J, Fu H Z. J Alloys Compd, 2012; 541: 275
|
[12] |
Allen D J, Hunt J D. Metall Trans, 1976; 7A: 767
|
[13] |
Liu D M, Su Y Q, Li X Z, Luo L S, Guo J J, Fu H Z. J Cryst Growth, 2010; 312: 3658
|
[14] |
Liu C. PhD Dissertation, Harbin Institute of Technology, 2006
|
[14] |
(刘 畅. 哈尔滨工业大学博士学位论文, 2006)
|
[15] |
Luo W Z, Shen J, Li Q L, Man W W, Fu H Z. Acta Metall Sin, 2007; 43: 897
|
[15] |
(罗文忠, 沈 军, 李庆林, 满伟伟, 傅恒志. 金属学报, 2007; 43: 897)
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|