低合金马氏体钢中的ω相 |
平德海1),殷匠2),刘文庆3),宿彦京4),戎利建5),赵新青6)
|
1) 中国石油大学(北京)材料科学与工程系,北京 102249
2) 江苏亚星锚链股份有限公司, 靖江 214533
3) 上海大学微结构重点实验室, 上海200444
4) 北京科技大学材料科学与工程学院, 北京 100083
5) 中国科学院金属研究所, 沈阳 110016
6) 北京航空航天大学材料科学与工程学院, 北京 100191 |
|
THE ω PHASE IN A LOW ALLOY MARTENSITIC STEEL |
PING Dehai1), YIN Jiang2), LIU Wenqing3), SU Yanjing4), RONG Lijian5), ZHAO Xinqing 6) |
1) Department of Materials Science and Engineering, China University of Petroleum, Beijing 102249
2) Jiangsu Asian Star Anchor Chain Co. Ltd., Jingjiang
3) Key Laboratory for Microstructure,Shanghai University, Shanghai 200444
4) School of Materials Science and Engineering, University of Science and
Technology Beijing, Beijing 100083
5) Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016
6) School of Materials Science and Engineering, Beihang University, Beijing 100191 |
引用本文:
平德海,殷匠,刘文庆,宿彦京,戎利建,赵新青. 低合金马氏体钢中的ω相[J]. 金属学报, 2013, 49(7): 769-774.
PING Dehai,
YIN Jiang,
LIU Wenqing,
SU Yanjing,
RONG Lijian,
ZHAO Xinqing.
THE ω PHASE IN A LOW ALLOY MARTENSITIC STEEL[J]. Acta Metall Sin, 2013, 49(7): 769-774.
[1]Frost P D, Parris W M, Hirsch L L, Doig J R, Schwartz C M.Trans Am Soc Met , 1954; 46: 231
[2]Hatt B A, Roberts J A, Williams G I. Nature, 1957; 180: 1406
[3]Sikka S K, VohraY K, ChidambaramR. Prog Mater Sci,1982; 27: 245
[4]Al-Zain Y, Kim H Y, Koyano T, Hosoda H, Namc T H, MiyazakiS. Acta Mater, 2011; 59: 1464
[5]Cui C Y, Ping D H. J Alloys Compd, 2009; 471: 248
[6]Lutjering G, Williams J C. Titanium. 2nd Ed.,Berlin: Springer-Verlag, 2007: 15
[7]Hatt B A, Roberts J A. Acta Metall, 1960; 8: 575
[8]Shao G, Tsakiropoulos P. Acta Mater, 2000; 48:3671
[9]Yedneral A F, Perkas M D. Phys Met Metall, 1972;33: 89
[10]Burakovsky L, Chen S P, Preston D L, Belonoshko A B,Mikhaylushkin A S, Simak S I, Moriarty J A. Phys Rev Lett, 2010; 104: 255702
[11]Cheng G M, Yuan H, Jian W W, Xu W Z, Millett P C, Zhu Y T.Scr Mater, 2013; 68: 130
[12]Baker H. Alloy Phase Diagrams. ASM Handbook, Vol.3, Washington D.C.: ASM International, 1992: 527
[13]Lee H Y, Yen H W, Chang H T, Yang J R. Scr Mater,2010; 62: 670
[14]Leslie W C, Hornbogen E. In: Cahn R W, Haasen P eds., Physical Metallurgy. 4th Ed, Amsterdam: Elsevier Science B V,1996: 1555
[15]Bhadeshia H K D H, Honeycombe S R. Steel Microstructure and Properties. 3rd Ed, Amsterdam: Elsevier, 2006: 1
[16]Lerchbacher C, Zinner S, Leitner H. Micron, 2012; 43: 818
[17]Ping D H, Geng W T. Mater Chem Phys, 2013; 139:830
[18]Nuttall K, Faulkner D. J Nucl Mater, 1977; 67:131
[19]Banerjee S, Mukhopadhyay P. Phase Transformations:Examples from Ti and Zr Alloys. Amsterdam: Elsevier, 2007: 473 |
|