| Ni2MnGa合金相界面位错结构及马氏体相变晶体学研究 |
| 韦昭召,马骁,张新平 |
| 华南理工大学材料科学与工程学院, 广州 510640 |
|
| STUDY ON THE DISLOCATION STRUCTURE OF INTERPHASE INTERFACE AND MARTENSITE TRANSFORMATION CRYSTALLOGRAPHY IN Ni2 MnGa ALLOY |
| WEI Zhaozhao, MA Xiao, ZHANG Xinping |
| School of Materials Science and Engineering, South China University of Technology, Guangzhou 510640 |
引用本文:
韦昭召,马骁,张新平. Ni2MnGa合金相界面位错结构及马氏体相变晶体学研究[J]. 金属学报, 2013, 49(2): 187-198.
WEI Zhaozhao,
MA Xiao,
ZHANG Xinping.
STUDY ON THE DISLOCATION STRUCTURE OF INTERPHASE INTERFACE AND MARTENSITE TRANSFORMATION CRYSTALLOGRAPHY IN Ni2 MnGa ALLOY[J]. Acta Metall Sin, 2013, 49(2): 187-198.
| [1] Ullakko K, Huang J K, Kanter C, Kokorin V V, O’Handley R C. Appl Phys Lett, 1996; 69: 1966 [2] Dunand D C, Mullner P. Adv Mater, 2011; 23: 216 [3] Ma Y Q, Jiang C B, Li Y, Xu H B, Wang C P, Liu X J. Acta Mater, 2007; 55: 1533 [4] Zhu F Q, Yang F Y, Chien C L, Ritchie L, Xiao G, Wu G H. J Magn Magn Mater, 2005; 288: 79 [5] Sasso C P, Zheng P Q, Basso V, Mullner P, Dunand D C. Intermetallics, 2011; 19: 952 [6] Chernenko V, Kohl M, Doyle S, Mullner P, Ohtsuka M. Scr Mater, 2006; 54: 1287 [7] Long Y, Zhang Z Y, Wen D, Wu G H, Ye R C, Chang Y Q, Wan F R. J Appl Phys, 2005; 98: 046102 [8] Zhao R B. PhD Thesis, Shanghai Jiao Tong University, 2003. (赵容斌. 上海交通大学博士论文, 2003) [9] Wayman C M. Introduction to the Crystallography of Martensite Transformation. New York: MacMillan, 1964 [10] Cong D Y, Zhang Y D, Wang Y D, Humbert M, Zhao X, Watanabe T, Zuo L, Esling C. Acta Mater, 2007; 55: 4731 [11] Cong D Y, Zetterstrom P, Wang Y D, Delaplane R, Peng R L, Zhao X, Zuo L. Appl Phys Lett, 2005; 87: 111906 [12] Rigsbee J M, Aaronson H I. Acta Metall, 1979; 27: 351 [13] Qiu D, Zhang W Z. Acta Metall Sin, 2006; 42: 341 (邱冬, 张文征. 金属学报, 2006; 42: 341) [14] Zhang W Z, Weatherly G C. Prog Mater Sci, 2005; 50: 181 [15] Weatherly G C, Zhang W Z. Metall Mater Trans, 1994; 25A: 1865 [16] Moritani T, Miyajima N, Furuhara T, Maki T. Scr Mater, 2002; 47: 193 [17] Pond R C, Celotto S, Hirth J P. Acta Mater, 2003; 54: 5385 [18] Pond R C, Ma X, Chai Y W, Hirth J P. Topological Modelling of Martensitic Transformations. In: Nabarro F R N, Hirth J P, eds., Dislocation in Solids, Amsterdam: Elsevier, 2007: 225 [19] Ma X, Pond R C. J Mater Sci, 2011; 46: 4236 [20] Ma X, Pond R C. Mater Sci Eng, 2008; A481-482: 404 [21] Chiao Y H, Chen I W. Acta Metall et Mater, 1990; 38: 1163 [22] Otsuka K, Wayman C M. Shape Memory Materials. Cambridge: Cambridge University Press, 1998: 4 [23] Ogawa K, Kajiwara S. Philos Mag, 2004; 84: 2919 [24] Olson G B, Cohen M. Acta Metall, 1979; 27: 1907 [25] Bilby B A, Bullough R, Smith E. Proc Roy Soc, 1955; 231: 263 [26] Frank F C. The Resultant Content of Dislocation in an Arbitrary Intercrystalline Boundary, In: Symposium on the Plastic Deformation of Crystalline Solid, Washington, D.C: U.S. Govt. Print. Off, 1950: 150 [27] Pond R C, Ma X, Hirth J P. Mater Sci Eng, 2006; A438-440: 109 [28] Zhang X M, Li D F, Xing Z S, Gautier E, Zhang J S, Simon A. Acta Metall et Mater, 1993; 41: 1693 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|