| 显微组织对新型热轧纳米析出强化钢断裂韧性的影响 |
| 孙茜1),王晓南2),章顺虎2),杜林秀3),邸洪双3) |
| 1) 沈阳飞机工业(集团)有限公司, 沈阳110034
2) 苏州大学沙钢钢铁学院, 苏州215021
3) 东北大学轧制技术及连轧自动化国家重点实验室, 沈阳110819 |
|
| EFFECT OF MICROSTRUCTURE ON FRACTURE TOUGHNESS OF NEW TYPE HOT—ROLLED NANO—SCALE PRECIPITATION STRENGTHENING STEEL |
| SUN Qian1), WANG Xiaonan2), ZHANG Shunhu2), DU Linxiu3), DI Hongshuang 3) |
| 1) Shenyang Aircraft Corporation, Shenyang 110034
2) Shagang School of Iron and Steel, Soochow University, Suzhou 215021
3) State Key Laboratory of Rolling and Automation, Northeastern University, Shenyang 110819 |
引用本文:
孙茜,王晓南,章顺虎,杜林秀,邸洪双. 显微组织对新型热轧纳米析出强化钢断裂韧性的影响[J]. 金属学报, 2013, 49(12): 1501-1507.
SUN Qian,
WANG Xiaonan,
ZHANG Shunhu,
DU Linxiu,
DI Hongshuang.
EFFECT OF MICROSTRUCTURE ON FRACTURE TOUGHNESS OF NEW TYPE HOT—ROLLED NANO—SCALE PRECIPITATION STRENGTHENING STEEL[J]. Acta Metall Sin, 2013, 49(12): 1501-1507.
| [1] Zhong Q P, Zhao Z H. Fractography. Beijing: Higher Education Press, 2006: 244
(钟群鹏, 赵子华. 断口学. 北京: 高等教育出版社, 2006: 244)
[2] Lacroix G, Pardoen T, Jacques P J. Acta Mater, 2008; 56: 3900
[3] Chen X, Li Y X, Fu H G. Acta Metall Sin, 2005; 41: 1061
(陈祥, 李言祥, 符寒光. 金属学报, 2005; 41: 1061)
[4] Bi Z Y, Yang J, Niu J, Zhang J X. Acta Metall Sin, 2013; 49: 576
(毕宗岳, 杨军, 牛靖, 张建勋. 金属学报, 2013; 49: 576)
[5] Firrao D, Matteis P, Spena P R, Gerosa R. Mater Sci Eng, 2013; A559: 371
[6] Seshu Kumar A, Ravi Kumar B, Datta G L, Ranganath V R. Mater Sci Eng, 2010; A527: 954
[7] Ren Z J, Ru C Q. Eng Fract Mech, 2013; 99: 214
[8] Fan Z Y. Mater Sci Eng, 1995; A191: 73
[9] Lai G Y, Wood W E, Clark R A, Zackay V F, Parker E R. Metall Mater Trans, 1974; 5B: 1663
[10] Shi Y W, Han Z X. J Mater Process Technol, 2008; 207: 30
[11] Kim S, Lee S, Lee B S. Mater Sci Eng, 2003; A359: 198
[12] Youngblood J L, Raghavan M. Metall Mater Trans, 1977; 8A: 1439
[13] Cao W D, Lu X P. Metall Mater Trans, 1987; 18A: 1569
[14] Ma Y, Pan T, Jiang B, Cui Y H, Su H, Peng Y.Acta Metall Sin, 2011; 47: 978
(马跃, 潘涛, 江波, 崔银会, 苏航, 彭云. 金属学报, 2011; 47: 978)
[15] Wang X N, Di H S, Du L X. Acta Metall Sin, 2012; 48: 621
(王晓南, 邸洪双, 杜林秀. 金属学报, 2012; 48: 621)
[16] Wang X N, Du L X, Di H S, Xie H, Gu D H. Steel Res Int, 2011; 82: 1417
[17] Zhong Y, Xiao F R, Zhang J W, Shan Y Y, Wang W, Yang K.Aata Mater, 2006; 54: 435
[18] Mills W J. J Test Eval, 1981; 9(1): 56
[19] Landes J D. Fatigue Fract Eng Mater Struct, 1995; 18: 1289
[20] Sakamoto H, Toyama K, Hirakawa K. Mater Sci Eng, 2000; A285: 288
[21] Fang H S, Liu D Y, Xu P G, Bai B Z, Yang Z G. Mater Mech Eng, 2001; 25: 1
(方鸿生, 刘东雨, 徐平光, 白秉哲, 杨志刚. 机械工程材料, 2001; 25: 1)
[22] Griffith A A. Philos Trans R Soc, 1920; 221A: 163
[23] Lee K H, Kim M C, Yang W J, Lee B S. Mater Sci Eng, 2013; A565: 158
[24] Qian C F, Jiang Z J, Chen P, Duan C H, Cui W Y. Acta Metall Sin, 2004; 40: 159
(钱才富, 姜忠军, 陈平, 段成红, 崔文勇. 金属学报, 2004; 40: 159)
[25] Xu J Q. Strength of Materials. Shanghai: Shanghai Jiao Tong University Press, 2009: 59
(许金泉. 材料强度学. 上海: 上海交通大学出版社, 2009: 59)
[26] Hwang B, Kim C G, Lee T. Metall Mater Trans, 2010; 41A: 85
[27] Byun J S, Shim J H, Cho Y W, Lee D N. Acta Mater, 2003; 51: 1593
[28] Yong Q L. Second Phases in Structural Steels. Beijing: Metallurgical Industry Press, 2006: 145
(雍岐龙. 钢铁材料中的第二相. 北京: 冶金工业出版社, 2006: 145)
[29] Deardo A J. In: Bordignon P J P, Carneiro T, Duncombe J eds.,The Fundamental Physical Metallurgy of Niobium in Steels. Warrendale: TMS, 2003: 427
[30] Wang X N, Du L X, Zhang H L, Di H S. J Iron Steel Res, 2011; 23(5): 45
(王晓南, 杜林秀, 张海仑, 邸洪双. 钢铁研究学报, 2011; 23(5): 45) |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|