| DD407单晶高温合金760℃屈服强度的LCP模型分析 |
| 张龙飞1,2),燕平1),赵京晨1),韩凤奎1),曾强1,2) |
| 1) 钢铁研究总院高温材料研究所, 北京 100081
2) 钢铁研究总院高温合金新材料北京重点实验室, 北京 100081 |
|
| ANALYZING THE YIELD STRENGTH OF SUPERALLOY SINGLE CRYSTAL DD407 AT 760℃ BY LCP-MODEL |
| ZHANG Longfei1, 2), YAN Ping1), ZHAO Jingchen1),HAN Fengkui1), ZENG Qiang1, 2) |
1) High Temperature Materials Research Department, Central Iron and Steel Research Institute,Beijing 100081
2) Beijing Key Laboratory of Advanced High Temperature Materials, Central Iron and Steel Research Institute, Beijing 100081 |
引用本文:
张龙飞,燕平,赵京晨,韩凤奎,曾强. DD407单晶高温合金760℃屈服强度的LCP模型分析[J]. 金属学报, 2013, 29(4): 489-494.
ZHANG Longfei,
YAN Ping,
ZHAO Jingchen,
HAN Fengkui,
ZENG Qiang.
ANALYZING THE YIELD STRENGTH OF SUPERALLOY SINGLE CRYSTAL DD407 AT 760℃ BY LCP-MODEL[J]. Acta Metall Sin, 2013, 29(4): 489-494.
| [1] Caron P, Khan T. Aerosp Sci Technol, 1999; 3: 5133 [2] Reed R C. The Superalloys Fundamentals and Applications. New York: Cambridge University Press, 2006: 121 [3] Hu Z Q, Liu L R, Jin T, Sun X F. Aeroengine, 2005; 31(3): 1 (胡壮麒, 刘丽荣, 金涛, 孙晓峰. 航空发动机, 2005; 31(3): 1) [4] Gunturi S S K, MacLachlan D W, Knowles D M. Mater Sci Eng, 2000; A289: 289 [5] Shah D M, Duhl D N. In: Beck G, Danesi W P, Gell M, Kent W B, Morrow H, Maurer G E, Miner R V,Ross E W, Stusrud R W, Tien J K, Wlodek S T eds., Superalloys 1984, Warrendale, PA: TMS, 1984: 105 [6] Miner R V, Voigt R C, Gayda J, Gabb T P. Metall Trans, 1986; 17A: 491 [7] Wang L N, Liu Y, Yu J J, Xu Y, Sun X F, Guan H R, Hu Z Q. Mater Sci Eng, 2009; A505: 144 [8] Osterle W, Bettge D, Fedelich B, Klingelhoffer H. Acta Mater,2000; 48: 689 [9] Takeuchi S, Kuramoto E. Acta Metall, 1973; 21: 415 [10] Lall C, Chin S, Pope D P. Metall Trans, 1979; 10A: 1323 [11] Miner R V, Voigt R C, Gayda J, Gabb T P. Metall Trans, 1986; 17A: 507 [12] Fang J F, Tian Z L, Yan P, Zhang J Y, Zheng Y. J Mater Eng, 2008; (3): 49 (方建锋, 田志凌, 燕平, 张晋远, 郑毅. 材料工程, 2008; (3): 49) [13] Guo Z Q, Fu T, Wang N, Fu H Z. J Inorg Mater, 2002; 17: 460 (郭振琪, 付涛, 王宁, 傅恒志. 无机材料学报, 2002; 17: 460) [14] Ha K F. Microscopic Theory of Mechanical Properties of Metals.Beijing: Science Press, 1983: 7 (哈宽富. 金属力学性质的微观理论. 北京: 科学出版社, 1983: 7) [15] Nembach E, Nitz A. Intermetallics, 1999; 7: 1383 [16] Copley S M, Kear B H, Rowe G M. Mater Sci Eng, 1972; 10: 87 [17] Nembach E, Neite G. Prog Mater Sci, 1985; 29: 177 [18] Nitz A, Nembach E. Acta Mater, 1998; 46: 4769 |
|