Hf含量对镍基粉末高温合金中γ'相形态的影响 |
张义文1,2,王福明1,胡本芙3 |
1. 北京科技大学冶金与生态工程学院, 北京 100083
2. 钢铁研究总院高温材料研究所, 北京 100081
3. 北京科技大学材料科学与工程学院, 北京 100083 |
|
EFFECT OF HAFNIUM CONTENT ON MORPHOLOGY EVOLUTION OF γ′ PRECIPITATES IN P/M Ni–BASED SUPERALLOY |
ZHANG Yiwen 1,2, WANG Fuming 1, HU Benfu 3 |
1. School of Metallurgical and Ecological Engineering, University of Science and Technology Beijing, Beijing 100083
2. High Temperature Material Institute, Central Iron and Steel Research Institute, Beijing 100081
3. School of Materials Science and Engineering, University of Science and Technology Beijing, Beijing 100083 |
引用本文:
张义文 王福明 胡本芙. Hf含量对镍基粉末高温合金中γ'相形态的影响[J]. 金属学报, 2012, 48(8): 1011-1017.
,
,
.
EFFECT OF HAFNIUM CONTENT ON MORPHOLOGY EVOLUTION OF γ′ PRECIPITATES IN P/M Ni–BASED SUPERALLOY[J]. Acta Metall Sin, 2012, 48(8): 1011-1017.
[1] Maniar G N, Bridge J E. Metall Trans, 1971; 2: 95[2] Muzyka D R. Met Eng Q, 1971; 11: 12[3] Hu B F, Liu G Q, Wu K, Tian G F. Acta Metall Sin, 2012; 48: 257(胡本芙, 刘国权, 吴 凯, 田高峰. 金属学报, 2012; 48: 257)[4] Kotval P S, Venables J D, Calder R W. Metall Trans, 1972; 3: 453[5] Duhl D N, Sullivan C P. J Met, 1971; 23: 38[6] Dahl J M, Danesi W F, Dunn R G. Metall Trans, 1973; 4: 1087[7] Maslenkov S B, Burova N N, Khangulov V V. Met Sci Heat Treat, 1980; 22: 283[8] Miner R V. Metall Trans, 1977; 8A: 259[9] Khachaturyan A G, Airapetyan V M. Phys Status Solidi, 1974; 26: 611[10] Qiu Y Y. Acta Mater, 1996; 44: 4969[11] Yoo Y S. Scr Mater, 2005; 53: 81[12] Zhang Y W, Wang F M, Hu B F. Acta Metall Sin, 2012; 48: 187(张义文, 王福明, 胡本芙. 金属学报, 2012; 48: 187)[13] Lifshitz I M, Slyozov V V. J Phys Chem Solids, 1961; 19: 35[14] Khachaturyan A G, Semenovskaya S V, Morris Jr J W. Acta Metall, 1988; 36: 1563[15] Kaufman M J, Voorhees P W, Johnson W C, Biancaniello F S. Metall Mater Trans, 1989; 20A: 2171[16] Grosdidier T, Hazotte A, Simon A. Mater Sci Eng, 1998; A256: 183[17] Banerjee D, Banerjee R, Wang Y. Scr Mater, 1999; 41: 1023[18] Qiu Y Y. J Alloys Compd, 1998; 270: 145[19] Cha P R, Yeon D H, Chung S H. Scr Mater, 2005; 52: 1241[20] Miyazaki T, Imamura H, Kozakai T. Mater Sci Eng, 1982; 54: 9[21] Doi M, Miyazaki T, Wakatsuki T. Mater Sci Eng, 1984; 67: 247 |
|