| FGH4096粉末高温合金的再结晶形核机制 |
| 宁永权, 姚泽坤 |
| 西北工业大学材料学院, 西安 710072 |
|
| RECRYSTALLIZATION NUCLEATION MECHANISM OF FGH4096 POWDER METALLURGY SUPERALLOY |
| NING Yongquan, YAO Zekun |
| School of Material Science and Engineering, Northwestern Polytechnical University, Xi’an 710072 |
引用本文:
宁永权 姚泽坤. FGH4096粉末高温合金的再结晶形核机制[J]. 金属学报, 2012, 48(8): 1005-1010.
.
RECRYSTALLIZATION NUCLEATION MECHANISM OF FGH4096 POWDER METALLURGY SUPERALLOY[J]. Acta Metall Sin, 2012, 48(8): 1005-1010.
| [1] Humphreys F J, Hatherly M. Recrystallization and Related Annealing Phenomena. 2nd Ed., Oxford: Elseriver, 2004: 10[2] Ning Y Q, Yao Z K, Fu M W, Guo H Z. Mater Sci Eng, 2011; A528: 8065[3] Ning Y Q, Fu M W, Yao W. Mater Sci Eng, 2012; A539: 101[4] Ning Y Q, Yao Z K, Xie X H, Guo H Z, Tan L J, Tao Y. Acta Metall Sin, 2010; 45: 58(宁永权, 姚泽坤, 谢兴华, 郭鸿镇, 谭立军, 陶宇. 金属学报, 2010; 45: 58)[5] Ning Y Q, Yao Z K, Yue TW, Guo H Z, Tao Y, Zhang Y W. Rare Met Mater Eng, 2010; 39: 1235(宁永权, 姚泽坤, 岳太文, 郭鸿镇, 陶 宇, 张义文. 稀有金属材料与工程, 2010; 39: 1235)[6] Reed R C. The Superalloys Fundamentals and Applications. New York: Cambridge University Press, 2006: 6[7] Ning Y Q, Yao Z K, Guo H Z, Tao Y, Zhang Y W. Key Eng Mater, 2009; 407–408: 694[8] Zhao M L, Sun WR, Yang S L, Qi F, Guo S R, Hu Z Q. Acta Metall Sin, 2009; 45: 79(赵美兰, 孙文儒, 杨树林, 祈峰, 郭守仁, 胡壮麒. 金属学报, 2009; 45: 79)[9] Viswanathan G B, Sarosi P M, Henry M F, Whitis D D, Milligan W W, Mills M J. Acta Mater, 2005; 53: 3041[10] Tiley G, Viswanathan G B, Srinivasan R, Banerjee R, Dimiduk D M, Fraser H L. Acta Mater, 2009; 57: 2538[11] MacSleyne J, Uchic M D, Simmons J P, Graef M D. Acta Mater, 2009; 57: 6251[12] Dunlavy M A, Shivpuri R, Semiatin S L. Mater Sci Eng, 2003; A359: 210[13] Viswanathan G B, Sarosi P M, Whitis D H, Mills M J. Mater Sci Eng, 2005; A400–401: 489[14] Cao F L, Qing H, Gu Y X, Guan C B, Zhou Q. Gas Turbine Exp Res, 2007; 20(3): 15(曹凤兰, 卿华, 古远兴, 关长波, 周全. 燃气涡轮试验与研究, 2007; 20(3): 15)[15] Liu F J, Zhang M C, Dong X, Zhang Y W. Acta Metall Sin (Engl Lett), 2007; 20: 102[16] Zhou X M, Wang W X, Tang D Z, Yan M G. Mater Eng, 2006; (11): 53(周晓明, 汪武祥, 唐定中, 颜鸣皋. 材料工程, 2006; (11): 53)[17] Liu J T, Liu G Q, Hu B F, Song Y P, Qin Z R, Zhang Y W. J Univ Sci Technol Beijing, 2006; 13: 319[18] Tian G F, Jia C C, Wen Y, Hu B F. J Univ Sci Technol Beijing, 2008; 15: 729[19] Ning Y Q, Yao Z K, Li H, Guo H Z, Tao Y, Zhang Y W. Mater Sci Eng, 2010; A527: 961[20] Ning Y Q, Yao Z K, Li H, Guo H Z, Tao Y, Zhang Y W. Chin J Mech Eng, 2009; 22: 925[21] Ning Y Q, Yao Z K, Fu M W, Guo H Z. Mater Sci Eng, 2010; A527: 6968[22] Xie X H, Yao Z K, Ning Y Q, Guo H Z, Tao Y, Zhang Y W. J Aero Mater, 2011; 31: 22(谢兴华, 姚泽坤, 宁永权, 郭鸿镇, 陶 宇, 张义文. 航空材料学报, 2011; 31: 22)[23] Ozols A, Sirkin H R, Vicente E E. Mater Sci Eng, 1999; A262: 64[24] Sun X Y, Song H M, Lin Q. J Chin Soc Rare Earths, 2004; 22: 177(孙学义, 宋红梅, 林勤. 中国稀土学报, 2004; 22: 177)[25] Yang P, Fu Y Y, Cui Y E. Acta Metall Sin, 2001; 37: 601(杨平, 傅云义, 崔月娥. 金属学报, 2001; 37: 601)[26] Yi M, Xiong H B, Lin Z. Shougang Sci Technol, 2008; (1): 1(易敏, 熊化冰, 林志. 首钢科技, 2008; (1): 1) |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|