| 镍基粉末冶金高温合金中γ'相形态不稳定性研究 |
| 胡本芙1), 刘国权1, 2), 吴凯1), 田高峰1) |
1) 北京科技大学材料科学与工程学院, 北京 100083
2) 北京科技大学新金属材料国家重点实验室, 北京 100083 |
|
| MORPHOLOGICAL INSTABILITY OF γ' PHASE IN NICKEL-BASED POWDER METALLURGY SUPERALLOYS |
| HU Benfu1), LIU Guoquan1, 2), WU Kai1), TIAN Gaofeng1) |
1) School of Materials Science and Engineering, University of Science and Technology Beijing, Beijing 100083
2) State Key Laboratory for Advanced Metals and Materials, University of Science and Technology Beijing, Beijing 100083 |
引用本文:
胡本芙 刘国权 吴凯 田高峰. 镍基粉末冶金高温合金中γ'相形态不稳定性研究[J]. 金属学报, 2012, 48(3): 257-263.
,
,
,
.
MORPHOLOGICAL INSTABILITY OF γ' PHASE IN NICKEL-BASED POWDER METALLURGY SUPERALLOYS[J]. Acta Metall Sin, 2012, 48(3): 257-263.
| [1] Doi M, Miyazaki T, Wakatsuki T. Mater Sci Eng, 1984; 67: 247[2] Doi M, Miyazaki T, Wakatsuki T. Mater Sci Eng, 1985; 74: 139[3] Qiu Y Y. J Alloy Compd, 1998; 270: 145[4] Leo P H, Lowengrub T S. Acta Mater, 2001; 49: 2761[5] Lee J K. Theor Appl Fract Mech, 2000; 33: 207[6] Yang A, Xiong Y, Liu L. Sci Technol Adv Mater, 2001; 2: 105[7] Banerjee D, Banerjee R, Wang Y. Scr Mater, 1999; 41: 1023[8] Li D Y, Chen L Q. Acta Mater, 1999; 47: 247[9] Cha P R, Yeon D H. Chung S H. Scr Mater, 2005; 52: 1241[10] Khachaturyan A G, Semenovskaya S V, Morris Jr J W. Acta Metall, 1988; 36: 1563[11] Yoo Y S. Scr Mater, 2005; 53: 81[12] Radis R, Schaffer M. Superalloy 2008, Warrendale, PA: TMS, 2008: 829[13] Furrer D. Scr Mater, 1999; 40: 1215[14] Qiu Y Y. Acta Mater, 1996; 44: 4969[15] Jackson M P, Reed R C. Mater Sci Eng, 1999; A259: 1241[16] Hazotte A, Grosdidier T, Denis S. Scr Mater, 1996; 34(4): 60[17] Gerold V, translated by Wang P X et al. Material Science and Technology: Solid Structre. Beijing: Science Press, 1998: 184(Gerold V著, 王佩璇等译. 材料科学与技术丛书: 固体结构. 北京: 科学出版社, 1998: 184)[18] Mullins W W, Sekerka R F. J Appl Phys, 1963; 34: 323[19] Ricks R A, Porter A J, Ecob R C. Acta Metall, 1983; 31: 43[20] Mitchell R J, Preuss M, Tin S, Hardy M C. Mater Sci Eng, 2008; A473: 158[21] Staron P, Kampmann R. Acta Mater, 2000; 48: 701[22] Staron P, Kampmann R. Acta Mater, 2000; 48: 713[23] Assadi H, Schroers J. Acta Mater, 2002; 50: 89 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|