| 晶粒尺寸对超低碳IF钢耐大气腐蚀性能的影响 |
| 汪兵,刘清友,王向东 |
| 钢铁研究总院结构材料研究所~ 先进钢铁流程及材料国家重点实验室, 北京 100081 |
|
| EFFECT OF GRAIN SIZE ON ATMOSPHERIC CORROSION RESISTANCE OF ULTRA--LOW CARBON IF STEEL |
| WANG Bing, LIU Qinyou, WANG Xiangdong |
| Institute for Structural Materials, State Key Laboratory of Advanced Steel Processing and Products, Central Iron and Steel Research Institute, Beijing 100081 |
引用本文:
汪兵,刘清友,王向东. 晶粒尺寸对超低碳IF钢耐大气腐蚀性能的影响[J]. 金属学报, 2012, 48(5): 601-606.
,
,
.
EFFECT OF GRAIN SIZE ON ATMOSPHERIC CORROSION RESISTANCE OF ULTRA--LOW CARBON IF STEEL[J]. Acta Metall Sin, 2012, 48(5): 601-606.
| [1] Weng Y Q. ISIJ Int, 2003; 43: 1675[2] Jouko I L. Adv Mater Process, 2001; 159: 31[3] Cao C N. Environmental Corrosion of Materials in China. Beijing: Chemistry Industry Press, 2005 (曹楚南. 中国材料的自然环境腐蚀. 北京: 化学工业出版社, 2005)[4] Youssef K M S, Koch C C, Fedkiw P S. Corros Sci, 2004; 46 (1): 51--64[5] Wislei R O, Celia M F, Amauri G. Mater Sci Eng, 2005; A402(1-2): 22--32[6] Di S A , Barteri M, Kenny J. J Mater Sci, 2003; 38(15): 3257--3262[7] Kalmykov V V, Razdobreev V G. Prot Met, 1999; 35(6): 598--599[8] Li Y, Wang F, Liu G. Corrosion, 2004; 60(10): 891--896[9] Wang B, Liu Q Y, Jia S J, Wang X D, Lu J, Dong H. J Chin Soc Corros Prot, 2007; 27(4): 193--196 (汪兵, 刘清友, 贾书君, 王向东, 卢吉, 董瀚. 中国腐蚀与防护学报, 2007; 27(4): 193--196)[10] Jiang P F, Wang B, Liu Q Y, Shi Z. Steel, 2009; 44(12): 67--70 (姜鹏飞, 汪兵, 刘清友, 施哲. 钢铁, 2009; 44(12): 67--70)[11] Mi F Y, Wang X D, Wang B, Chen X P, Peng Y. J Chin Soc Corros Prot, 2010; 30(5): 391--395 (米丰毅, 王向东, 汪兵, 陈小平, 彭云. 中国腐蚀与防护学报, 2010; 30(5): 391--395)[12] Li S P, Guo J, Yang S W, He X L. J Univ Sci Technol Beijing, 2008; 30(1): 16--20 (李少坡, 郭佳, 杨善武, 贺信莱. 北京科技大学学报, 2008; 30(1): 16--20)[13] Guo J, Yang S W, Shang C J, Wang Y, He X L. Corros Sci, 2009; 51: 242[14] Guo J, Yang S W, Shang C J, Wang Y, He X L. Iron Steel, 2008; 43: 58 (郭佳, 杨善武, 尚成嘉, 王郢, 贺信莱. 钢铁, 2008; 43: 58)[15] Sarkar P P, Kumar P, Manna M K, Charaborti P. Mater Lett, 2005; 59: 2488[16] Dong J, Cui W F, Zhang S X, Liu C M. J Northeastern Univ, 2007; 12: 1294 (董杰, 崔文芳, 张思勋, 刘春明. 东北大学学报, 2007; 12: 1294)[17] Fu G Y, Liu Q, Men B J, Zhang H L. Rare Met Mater Eng, 2007; 36: 695 (付广艳, 刘群, 门冰洁, 张宏亮. 稀有金属材料与工程, 2007; 36: 695)[18] Jin G Y, Qiao L J, Gao K W, Kimura T, Hashimoto K, Chu W Y. Chin J Nonferrous Met, 2004; 14: 210 (金光熙, 乔利杰, 高克玮, Kimura T, Hashimoto K, 褚武扬. 中国有色金属学报, 2004; 14: 210)[19] Qi J J, Huang Y H, Zhang Y. Microalloying Steel. Beijing: Metallurgical Industry Press, 2006: 10 (齐俊杰, 黄运华, 张跃. 微合金化钢. 北京: 冶金工业出版社, 2006: 10)[20] Cao C N, Zhang J Q. An Introduction to Electrochemical Impedance Spectroscopy.Beijing: Science Press, 2002: 188 (曹楚南, 张鉴清. 电化学阻抗谱导论. 北京: 科学出版社, 2002: 188)[21] Wang S T, Yang S W, Gao K W, Shen X A, He X L. Acta Metall Sin, 2008; 44: 1116 (王树涛, 杨善武, 高克玮, 沈晓安, 贺信莱. 金属学报, 2008; 44: 1116)[22] Bousselmi L, Fiaud C, Tribollet B, Triki E. Corros Sci, 1997; 39: 1711[23] Bousselmi L, Fiaud C, Tribollet B, Triki E. Electrochim Acta, 1999; 44: 4357[24] Santana Rodriguez J J, Santana Hernandez F J, Gonzalez J E. Corros Sci, 2002; 44: 2597[25] Yu Y N. Metallography. Bei Jjing: Metallurgical Industry Press, 2000: 375 (余永宁. 金属学. 北京: 冶金工业出版社, 2000: 375) |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|