| 不同La含量AZ91合金的时效硬化行为 |
| 张金玲1,2,3,冯芝勇1,胡兰青1,2,3,王社斌1,2,3,许并社1,2,3 |
1. 太原理工大学材料科学与工程学院, 太原 030024
2. 新材料界面科学与工程教育部重点实验室, 太原 030024
3. 山西省新材料工程技术研究中心, 太原 030024 |
|
| PRECIPITATION BEHAVIOR OF AZ91 MAGNESIUM ALLOYS WITH DIFFERENT La CONTENTS |
| ZHANG Jinling1,2,3, FENG Zhiyong1, HU Lanqing1,2,3,WANG Shebin1,2,3, XU Bingshe1,2,3 |
1. Taiyuan University of Technology, College of Material Science and Technology, Taiyuan 030024
2. Key Laboratory of Interface Science and Engineering in Advanced Materials, Ministry of Education, Taiyuan 030024
3. Shanxi Research Center of Advanced Materials Science and Technology,Taiyuan 030024 |
引用本文:
张金玲,冯芝勇,胡兰青,王社斌,许并社. 不同La含量AZ91合金的时效硬化行为[J]. 金属学报, 2012, 48(5): 607-614.
,
,
,
,
.
PRECIPITATION BEHAVIOR OF AZ91 MAGNESIUM ALLOYS WITH DIFFERENT La CONTENTS[J]. Acta Metall Sin, 2012, 48(5): 607-614.
| [1] Aghion E, Bronfin B, Eliezer D. J MaterProcess Technol,2001; 117: 381[2] Mordike B L, Ebert T. Mater Sci Eng, 2001; A302: 37[3] Liu Q. Acta Metall Sin, 2010; 46: 1458 (刘庆. 金属学报, 2010; 46: 1458)[4] Chen Z H, Yan H G. Magnesium Alloy. Beijing: Chemical Industry Press, 2004, 29 (陈振华, 严红革. 镁合金. 北京: 化学工业出版社, 2004, 29)[5] Clark J B, Zabdyr L, Moser Z. In: ASM Handbook, vol.3, Alloy Phase Diagrama. Materials Park, Ohio: ASM International, 1992: 285[6] Zeng X Q, Wu Y J, Peng L M. Acta Metall Sin, 2010; 46: 1041 (曾小勤, 吴玉娟, 彭立明. 金属学报, 2010; 46: 1041)[7] Xiao X L, Luo C P, Liu J W, Wu D X, Nie J F. Chin J Nonferrous Met,2003; 13: 15 (肖晓玲, 罗承萍, 刘江文, 吴东晓, 聂建峰. 中国有色金属学报, 2003; 13: 15)[8] Xiao X L, Luo C P, Nie J F. Acta Metall Sin, 2001; 37: 1 (肖晓玲, 罗承萍, 聂建峰. 金属学报, 2001; 37: 1)[9] Xiao X L, Luo C P, Liu J W, Nie J F. Acta Metall Sin, 2002; 28: 709 (肖晓玲, 罗承萍, 刘江文, 聂建峰. 金属学报, 2002; 28: 709)[10] Cizek L, Greger M, Pawlica L, Dobrzanski L A, Tanski T.J Mater Process Technol, 2004; 157--158: 466[11] Li P J, Tang B, Kandal ova E G. Mater Lett, 2005; 59: 671[12] Zhao Y H, Chen Y G, Tang Y B. Rare Met Mater Eng, 2010; 39: 843 (赵源华, 陈云贵, 唐永柏. 稀有金属材料与工程, 2010; 39: 844)[13] Zhang J L, Wang S B, Xu B S. Rare Met Mater Eng, 2007; 36: 1061 (张金玲, 王社斌, 许并社. 稀有金属材料与工程, 2007; 36: 1061)[14] Li W X. Magnesium and Magnesium Alloy. Changsha: Central South University Press, 2005; 341 (黎文献. 镁及镁合金. 长沙: 中南大学出版社, 2005; 341)[15] Tang W, Han E H, Xu Y B. Acta Metall Sin, 2005, 41: 1199 (唐伟, 韩恩厚, 徐永波. 金属学报, 2005; 41: 1199)[16] Zhang J M, Jiang B L, Wang Z H, Yuan S, Xia P J. Heat Treat Met,2007; 32: 6 (张菊梅, 蒋百灵, 王志虎, 袁森, 夏鹏举. 金属热处理, 2007; 32: 6)[17] Wang S B, Qi X Y, Zhang J L, Xu B S. Acta Metall Sin, 2011; 47: 743 (王社斌, 祁小叶, 张金玲, 许并社. 金属学报, 2011; 47: 743)[18] Wu Y R. PhD Thesis, Hunan University, Changsha, 2007 (吴玉蓉. 湖南大学博士论文, 长沙, 2007)[19] Liu L F, Ding H L, Ding W J. Rare Met Mater Eng, 2009; 38: 104 (刘六法, 丁汉林, 丁文江. 稀有金属材料与工程, 2009; 38: 104)[20] Yu K, Li W X, Zhang S J. Rare Met Mater Eng, 2005; 34: 1105 (余琨, 黎文献, 张世军. 稀有金属材料与工程, 2005; 34: 1105)[21] Wang S B, Zhang J L, Qi X Y, Xu B S. Mater Eng, 2009; (Suppl.1): 303 (王社斌, 张金玲, 祁小叶, 许并社. 材料工程, 2009; (增刊1): 303) |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|