| P92钢焊接接头IV型蠕变断裂特性 |
| 王学,潘乾刚,陶永顺,章应霖,曾会强,刘洪 |
1. 武汉大学动力与机械学院, 武汉 430072
2. 东方电气集团东方锅炉股份有限公司, 自贡 643001 |
|
| TYPE IV CREEP RUPTURE CHARACTERISTICS OF P92 STEEL WELDMENT |
| WANG Xue1, PAN Qiangang2, TAO Yongshun2, ZHANG Yinglin1,ZENG Huiqiang2,LIU Hong2 |
1. School of Power and Mechanics, Wuhan University, Wuhan 430072
2. Dongfang Electric Corporation, Dongfang Boiler Group Co Ltd., Zigong 643001 |
引用本文:
王学,潘乾刚,陶永顺,章应霖,曾会强,刘洪. P92钢焊接接头IV型蠕变断裂特性[J]. 金属学报, 2012, 48(4): 427-434.
,
,
,
,
,
.
TYPE IV CREEP RUPTURE CHARACTERISTICS OF P92 STEEL WELDMENT[J]. Acta Metall Sin, 2012, 48(4): 427-434.
| [1] Jorgen B, Sven K, Rudolph B. Energy, 2006; 31: 1437[2] Richardot D, Vaillant J C, Arbab A, Bendick W. The T92/P92 steel book. 2nd Ed. Boulogne: Vallourec & Mabbesmann tubes, 2002[3] Shen Q, Liu H G. Electr Power Constrc, 2010; 31: 71 (沈琦, 刘鸿国. 电力建设, 2010, 31: 71)[4] Tu S D, Xuan F Z, Wang W Z. Acta Metall Sin, 2009; 45: 781 (涂善东, 轩福贞, 王卫泽. 金属学报, 2009, 45: 781)[5] Scheller H J, Haigh L, Woitscheck A. Der Mascginenschaden,1974; 47: 1[6] Laha K, Chandravathi K S, Rao K B S, Mannan S L, Sastry D H. Metall MaterTrans, 2001; 32A: 115[7] Tabuchi M, Watanabe T, Kubo K, Matsui M, Kinugawa J, Abe F. J Pressure Vessel Pip, 2001; 78: 779[8] Kojima T, Hayashi K, Kajita Y. ISIJ Int, 1995; 35: 1284[9] Matsui M, Tabuchi M, Watanabe T, Kubo K. ISIJ Int, 2001; 41: S126[10] Li D J, Shinozaki K, Kuroki H. Sci Technol Weld Join, 2003; 8: 296[11] Abd El--Azim M E, Nasreldin A M, Zies G, Klenk A. Mater Sci Technol, 2005; 21: 779[12] Watanabe T, Tabuchi M, Yamazaki M, Hongo H, Tanabe T. J Pressure Vessel Pip, 2006; 83: 63[13] Albert S K, Matsui M, Watanabe T, Hongo H, Kubo K. J Pressure Vessel Pip, 2003; 80: 405[14] Korcakova L, Hald J. Mater Charact, 2001; 47: 111[15] Qin G Y. Quality Metallography. Chendu: Sichuan Publishing House of Science and Technology, 1987: 1 (秦国友. 定量金相. 成都: 四川科学技术出版社, 1987: 1)[16] Chen B L. Imperfection Analysis and Countmeasures for Welding Engineering. Beijing: China Machine Press, 2006: 301 (陈伯蠡. 焊接工程缺欠分析与对策. 北京: 机械工业出版社, 2006: 301)[17] Zhang J S. High Temperature Deformation and Fracture of Materials. Beijing: Science Press, 2007: 378 (张俊善. 材料的高温变形与断裂. 北京: 科学出版社, 2007: 378)[18] Robertson D G, Holdsworth S R. ECCC Data Sheets 2005. UK: ETD Ltd., 2005: 47[19] Maruyama K, Sawada K, Koike J. ISIJ Int, 2001; 41: 641[20] Komai N, Masuyama F. ISIJ Int, 2002 ; 42: 1364[21] Gaffard V, Gourgues-Lorenzon A F, Besson J. Nucl Eng Des,2005; 235: 2547[22] Hald J, Korcakova L. ISIJ Int, 2003; 43: 420[23] Dimmler G, Weinert P, Kozeschnik E, Cerjak H. Mater Charact,2003; 51: 341[24] Hattestrand M, Andren H. Micron, 2001; 32: 789[25] Lee J S, Armaki H G, Maruyama K, Muraki T, Asahi H. Mater Sci Eng, 2006; A428: 270[26] Peng Z F, Cai L S, Peng F F, Hu Y P, Chen F Y. Acta Metall Sin,2010; 46: 429 (彭志方, 蔡黎胜, 彭芳芳, 胡永平, 陈方玉. 金属学报, 2010, 46: 429)[27] Li D J, Shinozaki K. Sci Technol Weld Join, 2005; 10: 544[28] Smith D J, Walker N S, Kimmins S T. J Pressure Vessel Pip,2003; 80: 617 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|