| 强变形对Cu-Cr合金组织性能的影响 |
| 宋鲁男1,刘嘉斌1,2,黄六一1.3,曾跃武1,孟亮1 |
1. 浙江大学材料系, 杭州 310027
2. 浙江大学力学系, 杭州 310027
3. 浙江省特种设备检验研究院, 杭州 310015 |
|
| EFFECT OF HEAVILY DRAWING ON THE MICROSTRUCTURE AND PROPERTIES OF Cu–Cr ALLOYS |
| SONG Lunan 1, LIU Jiabin 1,2, HUANG Liuyi 1,3, ZENG Yuewu 1, MENG Liang 1 |
1) Department of Materials Science and Engineering, Zhejiang University, Hangzhou 310027
2) Department of Mechanics Science and Engineering, Zhejiang University, Hangzhou 310027
3) Zhejiang Special Equipment Inspection and Research Institute, Hangzhou 310015 |
引用本文:
宋鲁男 刘嘉斌 黄六一 曾跃武 孟亮. 强变形对Cu-Cr合金组织性能的影响[J]. 金属学报, 2012, 48(12): 1459-1466.
SONG Lunan LIU Jiabin HUANG Liuyi ZENG Yuewu MENG Liang.
EFFECT OF HEAVILY DRAWING ON THE MICROSTRUCTURE AND PROPERTIES OF Cu–Cr ALLOYS[J]. Acta Metall Sin, 2012, 48(12): 1459-1466.
| [1] Deng J Q, Zhang X Q, Shang S Z, Liu F, Zhao Z X, Ye Y F. Mater Des, 2009; 30: 4444[2] Wang X F, Zhao J Z, He J. Mater Sci Eng, 2007; A460: 69[3] Liu P, Kang B X, Cao X G, Huang J L, Gu H C. Acta Metall Sin, 1999; 35: 561(刘 平, 康布熙, 曹兴国, 黄金亮, 顾海澄. 金属学报, 1999; 35: 561)[4] Chbihi A, Sauvage X, Blavette D. Acta Mater, 2012; 60: 4575[5] West E G. Copper and its Alloys. Chichester: Ellis Horwood, 1982: 1[6] Fujii T, Nakazawa H, Kato M, Dahmen U. Acta Mater,2000; 48: 1033[7] Li Y, Chen X H, Liu P, Gao L H, Tian B H. Trans Mater Heat Treat, 2011; 32(2): 86(李 炎, 陈小红, 刘 平, 高林华, 田保红. 材料热处理学报, 2011; 32(2): 86)[8] Jin Y, Adachi K, Takeuchi T, Suzuki H G. J Mater Sci, 1998; 33: 1333[9] Jin Y, Adachi K, Takeuchi T, Suzuki H G. Mater Sci Eng, 1999; A212: 149[10] Liu J L, Wang E D, Liu Z Y, Hu L X, Fang W B. Mater Sci Eng, 2004; A382: 301[11] Liu J B, Zhang L, Yao D W, Meng L. Acta Mater, 2011; 59: 1191[12] Raabe D, Ohsaki S, Hono K. Acta Mater, 2009; 57: 5254[13] Zhang D L, Mihara K, Takakura E, Suzuki H G. Mater Sci Eng, 1999; A296: 99[14] Liu Y, Shao S, Liu K M, Yang X J, Lu D P. Mater Sci Eng, 2012; A531: 141[15] Jin Y, Adachi K, Takeuchi T, Suzuki H G. Metals Mater Trans, 1998; 29A: 2195[16] Sinclair C W, Embury J D, Weatherly G C. Mater Sci Eng, 1999; A272: 90[17] Sun S J, Sakai S, Suzuki H G. Mater Trans, 2000; 41: 613[18] Wang Y L, Han K, Huang Y, Zhang K Y. Mater Sci Eng, 2003; A351: 214[19] Snoeck E, Lecouturier F, Thilly L, Casanove M J, Rakoto H, Coffe G, Askenazy S, Peyrade J P, Roucou C, Pantsyrny V, Shikov A, Nikulin A. Scr Mater, 1998; 38: 1643[20] Liu K M, Lu D P, Zhou H T, Atrens A, Chen Z B, Zou J, Zeng S M. J Alloys Compd, 2010; 500: L22[21] Lee K L, Whitehouse A F, Russell A M, Wongpreedee K, Hong S I, Withers P J. J Mater Sci, 2003; 38: 3437[22] Wingrove A L. J Inst Met, 1972; 100: 313[23] Cairns J H, Clough J, Dewey M, Nutting J. J Inst Met, 1971; 99: 93[24] Lee T C, Robertson I M, Birnbaum H K. Ultramicroscopy, 1989; 29: 212[25] Zhang L, Meng L. Chin J Nonferrous Met, 2005; 15: 751(张雷, 孟亮. 中国有色金属学报, 2005; 15: 751)[26] Heringhaus F, Schneider–Muntau H J, Gottstein G. Mater Sci Eng, 2003; A347: 9 |
|