| HCO3-和Cl-混合体系中Cu的点蚀行为研究 |
| 王长罡, 董俊华, 柯伟, 陈楠, 李晓芳 |
| 中国科学院金属研究所金属腐蚀与防护国家重点实验室, 沈阳 110016 |
|
| RESEARCH ON PITTING CORROSION BEHAVIOR OF COPPER IN THE SOLUTION WITH HCO3- AND Cl- |
| WANG Changgang, DONG Junhua, KE Wei, CHEN Nan, LI Xiaofang |
| State Key Laboratory for Corrosion and Protection, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016 |
引用本文:
王长罡 董俊华 柯伟 陈楠 李晓芳. HCO3-和Cl-混合体系中Cu的点蚀行为研究[J]. 金属学报, 2012, 48(11): 1365-1373.
WANG Changgang DONG Junhua KE Wei CHEN Nan LI Xiaofang.
RESEARCH ON PITTING CORROSION BEHAVIOR OF COPPER IN THE SOLUTION WITH HCO3- AND Cl-[J]. Acta Metall Sin, 2012, 48(11): 1365-1373.
| [1] Wang C G, Dong J H, Ke W, Chen N. Acta Metall Sin, 2011; 47: 354(王长罡, 董俊华, 柯 \ \ 伟, 陈楠, 金属学报, 2011; 47: 354)[2] Darren A, Lytle A, Mallikarjuna N, Nadagouda B. Corros Sci, 2010; 52: 1927[3] Guo Y H, Wang J, Wang ZM, Liu S F, Su Y. Bull Mineral Petrol Geochem, 2007; 26: 607(郭永海, 王 驹, 王志明, 刘淑芬, 苏 锐. 矿物岩石地球化学通报, 2007; 26: 607)[4] Fujii T, Kodama T, Baba H. Corros Sci, 1984; 24: 901[5] Drogowska M, Brossard L, M´enard H. Surf Coat Technol, 1988; 34: 383[6] Drogowska M, Brossard L, M´enard H. J Electrochem Soc, 1992; 139: 39[7] Duthil J P, Mankowski G, Giusti A. Corros Sci, 1996; 38: 1839[8] Reda M R, Alhajji J N. Corrosion, 1996; 52: 232[9] Cantor A F, Park J K, Vaiyavatjamai P. J Am Water Works Assoc, 2003; 95(5): 112[10] Baba H, Kodama T, Fujii T. Trans Natl Res Inst Met, 1986; 28: 248[11] Christy A G, Lowe A, Otieno–Alego V, Stoll M, Webster R D. J Appl Electrochem, 2004; 34: 225[12] Edwards M, Ferguson J F, Reiber S H. J AmWaterWorksAssoc, 1994; 86(7): 74[13] Sosa M, Patel S, Edwards M. Corrosion, 1999; 55: 1069[14] Edwards M, Rehring J, Mayer T. Corrosion, 1994; 50: 366[15] Cong H, Scully J R. J Electrochem Soc, 2010; 157: C200[16] Nishikata A, Itagaki M, Tsuru T, Haruyama S. Corros Sci, 1990; 31: 287[17] Jujii T. Trans Natl Res Inst Met, 1988; 30(2): 81[18] Drogowska M, Brossard L, M´enard H. J Electrochem Soc, 1992; 139: 39[19] Wang C G, Dong J H, Ke W, Chen N. Acta Metall Sin, 2012; 48: 85(王长罡, 董俊华, 柯伟, 陈 楠. 金属学报, 2012; 48: 85)[20] Abd El Meguid E A, Awad N K. Corros Sci, 2009; 51: 1134[21] Ding J, Lin H C, Cao C N. Corros Sci Prot Technol, 2002; 14: 67(丁杰, 林海潮, 曹楚南. 腐蚀科学与防护技术, 2002; 14: 67) |
|