| 硼酸缓冲溶液中pH值和Cl-浓度对Cu腐蚀行为的影响 |
| 王长罡, 董俊华, 柯伟, 陈楠 |
| 中国科学院金属研究所金属腐蚀与防护国家重点实验室, 沈阳 110016 |
|
| EFFCTS OF pH AND Cl− CONCENTRATION ON THE CORROSION BEHAVIOR OF COPPER IN BORIC ACID BUFFER SOLUTION |
| WANG Changgang, DONG Junhua, KE Wei, CHEN Nan |
State Key Laboratory for Corrosion and Protection, Institute of Metal Research, Chinese Academy of Sciences,
Shenyang 110016 |
引用本文:
王长罡 董俊华 柯伟 陈楠. 硼酸缓冲溶液中pH值和Cl-浓度对Cu腐蚀行为的影响[J]. 金属学报, 2011, 47(3): 354-360.
,
,
,
.
EFFCTS OF pH AND Cl− CONCENTRATION ON THE CORROSION BEHAVIOR OF COPPER IN BORIC ACID BUFFER SOLUTION[J]. Acta Metall Sin, 2011, 47(3): 354-360.
| [1] Xu Q J, Wang W, Zhou G D. J Mater Prot, 2006; 39(7): 51(徐群杰, 王伟, 周国定. 材料保护, 2006; 39(7): 51)[2] Zhu X L, Lin L Y, Lei T Q. Acta Metall Sin, 1997; 33: 1256(朱小龙, 林乐耘, 雷廷权. 金属学报, 1997; 33: 1256)[3] Xu Q J, Zhu L J, Qi H, Cao W M, Zhou G D. Acta Metall Sin, 2008; 44: 1360(徐群杰, 朱律均, 齐航, 曹为民, 周国定. 金属学报, 2008; 44: 1360)[4] Smith J M, Wren J C, Dziemkowski M O, Shoesmith D W. J Electrochem Soc, 2007; 154: 431[5] Ding J, Lin H C, Cao C N. Corros Sci Prot Technol, 2002; 14: 67(丁杰, 林海潮, 曹楚南. 腐蚀科学与防护技术, 2002; 14: 67)[6] Trachli B, Keddam M, Takenouti H, Srhiri A. Corros Sci, 2002; 44: 997[7] Cicileo G, Rosales B, Varela F, Vilche J. Corros Sci, 1999; 41: 1359[8] Valcarce M, De Sanchez S, Vazquez M. J Mater Sci, 2006; 41: 1999[9] Srivastava A, Balasubramaniam R. Mater Charact, 2005; 55: 127[10] Palit A, Pehkonen S. Corros Sci, 2000; 42: 1801[11] Brizuela F, Procaccini R, Cere S, Vazquez M. J Appl Electrochem , 2006; 36: 583[12] Bech–Nielsen G, Jaskula M, Chorkendorff, Larsen J. Electrochim Acta, 2002; 47: 4279[13] Deslouis C, Tribollet B, Mengoli G, Musiani M M. J Appl Electrochem, 1988; 18: 374[14] Deslouis C, Tribollet B, Mengoli G, Musiani M M. J Appl Electrochem, 1988; 18: 384[15] Diard J P, Le Canut J M, Le Gorrec B, Montella C. Electrochim Acta, 1998; 43: 2485[16] Li D G, Feng Y R, Bai Z Q, Zhu J W, Zheng M S. Electrochim Acta, 2007; 52: 7877[17] Shinji F, Hiroaki T. Corros Sci, 2007; 49: 195 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|