| 医用Mg-Ca和Mg-Li-Ca合金腐蚀研究 |
| 曾荣昌1, 2, 3), 郭小龙2), 刘成龙2), 崔洪芝1), 陶武2), 刘云逸2), 李博文2) |
1) 山东科技大学材料科学与工程学院, 青岛 266590
2) 重庆理工大学材料科学与工程学院, 重庆 400050
3) 中国科学院金属研究所金属腐蚀与防护国家重点实验室, 沈阳 110016 |
|
| STUDY ON CORROSION OF MEDICAL Mg-Ca AND Mg-Li-Ca ALLOYS |
| ZENG Rongchang1, 2, 3), GUO Xiaolong2), LIU Chenglong2), CUI Hongzhi1), TAO Wu2), LIU Yunyi2), LI Bowen2) |
1) College of Materials Science and Engineering, Shandong University of Science and Technology, Qingdao 266590
2) School of Materials Science and Engineering, Chongqing University of Technology, Chongqing 400050
3) State Key Laboratory for Corrosion and Protection, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016 |
引用本文:
曾荣昌 郭小龙 刘成龙 崔洪芝 陶武 刘云逸 李博文. 医用Mg-Ca和Mg-Li-Ca合金腐蚀研究[J]. 金属学报, 2011, 47(11): 1477-1482.
,
,
,
,
,
.
STUDY ON CORROSION OF MEDICAL Mg-Ca AND Mg-Li-Ca ALLOYS[J]. Acta Metall Sin, 2011, 47(11): 1477-1482.
| [1] Zeng R C, Dietzel W, Witte F, Hort N. Adv Eng Mater, 2008; 10B: 3[2] Staiger M P, Pietak A M, Huadmai J, Dias G. Biomaterials, 2006; 27: 1728[3] Song G L. Corros Sci, 2007; 49: 1696[4] Witte F, Kaese V, Haferkamp H, Switzer E, Meyer–Lindenberg A, Wirth C J, Windhagen H. Biomaterials, 2005; 26: 3557[5] Hong Y S, Yang K, Zhang G D, Huang J J, Hao Y Q, Ai H J. Acta Metall Sin, 2008; 44: 1035(洪岩松, 杨柯, 张广道, 黄晶晶, 郝玉全, 艾红军. 金属学报, 2008; 44: 1035)[6] Zeng R C, Kong L H, Chen J, Cuo H Z, Liu C L. Chin J Nonferrous Met, 2011; 21: 35(曾荣昌, 孔令鸿, 陈君, 崔洪芝, 刘成龙. 中国有色金属学报, 2011; 21: 35)[7] Zhang J, Zong Y, Fu P H, Yuan G Y, Ding W J. J Clin Rehabil Tissue Eng Res, 2009; 13: 574(张佳, 宗阳, 付彭怀, 袁广银, 丁文江. 中国组织工程研究与临床康复, 2009; 13: 5747)[8] Zhang C Y, Gao J C, Zeng R C, Liu C L, Wu X, Wu D. J Chin Ceram Soc, 2010; 38: 885(张春艳, 高家诚, 曾荣昌, 刘成龙, 吴 霞, 吴迪. 硅酸盐学报, 2010; 38: 885)[9] Zhang C Y, Zeng R C, Liu C L, Gao J C. Surf Coat Technol, 2010; 204: 3636[10] Zhang C Y, Zeng R C, Chen J, Yang H, Tian Z Q. Rare Met Mater Eng, 2009; 38: 1363(张春艳, 曾荣昌, 陈君, 杨 惠, 田中青. 稀有金属材料与工程, 2009; 38: 1363)[11] Li Z, Gu X, Lou S, Zheng Y. Biomaterials, 2008; 29: 1329[12] Zberg B, Uggowitzer P J, Loeffler J F. Nature Mater, 2009; 8: 887[13] Ma E, Xu J. Nature Mater, 2009; 8: 855[14] Li J, Song Y, Zhang S, Zhao C, Zhang F, Zhang X, Cao L, Fan Q, Tang T. Biomaterials, 2010; 31: 5782[15] Zheng Y F, Liu B, Gu X N. Mater Rev, 2009; 7: 187(郑玉峰, 刘 彬, 顾雪楠. 材料导报, 2009; 7: 187)[16] Liu C L, Wang Y J, Zeng R C, Zhang X M, Huang W J, Chu P K. Corros Sci, 2010; 52: 3341[17] Bobby K M, Singh R R K. Biomaterials, 2008; 29: 2306[18] Zhang C Y, Zeng R C, Liu C I, Chen R S, Gao J C. Trans Nonferrous Met Soc China, 2010; 20(suppl): s655[19] Witte F, Fischer J, Nellesen J, Vogt C, Vogt J, Donath T, Beckmann F. Acta Biomater, 2010; 6: 1792[20] Leeflang M A, Zhou J, Duszczyk J. In: Kainer K U ed., Proceeding of 8th Int Conf Magnesium Alloys and Their Applications, Weinheim: Wiley, 2009: 1182[21] Zhang M L, Elkin F M. Magnesium–Lithium Superlight Alloys. Beijing: Science Press, 2010: 304(张密林, Elkin F M. 镁锂超轻合金. 北京: 科学出版社, 2010: 304)[22] Matucha K H, translated by Ding D Y. Structure and Properties of Nonferrous Alloys. Beijing: Science Press, 1999: 120(马图哈 K H, 丁道云 译. 非铁合金的结构与性能. 北京: 科学出版社, 1999: 120)[23] Sivashanmugam A, Kumar T P, Renganathan N G, Gopukumar S. J Appl Electrochem, 2004; 34: 1135[24] Lin M C, Tsai C Y, Uan J Y. Corros Sci, 2009; 51: 2463[25] Huang X M, Zhang C H, Zhang M L. J Aeronaut Mater, 2008; 28: 71(黄晓梅, 张春红, 张密林. 航空材料学报, 2008; 28: 71)[26] Zeng R C, Kong L H, Xu S, Zhang C Y, Wang M. J Chongqing Univ Technol, 2010; 24: 34(曾荣昌, 孔令鸿, 许苏, 张春艳, 王猛. 重庆理工大学学报, 2010; 24: 34)[27] Shi Z M, Liu M, Atrens A. Corros Sci, 2010; 52: 579[28] Grobner J, Schmid–Fetzer R, Pisch A, Colinet C, Pavlyuk V V, Dmytriv G S, Kevorkov D G, Bodak O I. Thermochim Acta, 2002; 389: 85[29] Li Z J, Gu X N, Lou S Q, Zheng Y F. Biomaterials, 2008; 29: 1329[30] Zeng R C, Chen J. Trans Nonferrous Met Soc China, 2007; 17(suppl): s193[31] Song Y W, Shan D Y, Chen R S, Han E H. Corros Sci, 2009; 51: 1087[32] Urquidi–Macdonald M, Macdonald D D, Pensado O, Flores J R. Electrochim Acta, 2001; 47: 833[33] Song Y W, Shan D Y, Chen R S, Zhang F, Han E H. Mater Sci Eng, 2009; C29: 1039 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|