| 抽拉速率对定向凝固叶片状DZ125高温合金微观组织的影响 |
| 葛丙明, 刘林, 张胜霞, 张军, 李亚峰, 傅恒志 |
| 西北工业大学凝固技术国家重点实验室, 西安 710072 |
|
| INFLUENCE OF WITHDRAWAL RATE ON MICROSTRUCTURES OF BLADE SHAPED DIRECTIONALLY SOLIDIFIED DZ125 SUPERALLOY |
| GE Bingming, LIU Lin, ZHANG Shengxia, ZHANG Jun, LI Yafeng, FU Hengzhi |
| State Key Laboratory of Solidification Processing, Northwestern Polytechnical University, Xi'an 710072 |
引用本文:
葛丙明 刘林 张胜霞 张军 李亚峰 傅恒志. 抽拉速率对定向凝固叶片状DZ125高温合金微观组织的影响[J]. 金属学报, 2011, 47(11): 1470-1476.
,
,
,
,
,
.
INFLUENCE OF WITHDRAWAL RATE ON MICROSTRUCTURES OF BLADE SHAPED DIRECTIONALLY SOLIDIFIED DZ125 SUPERALLOY[J]. Acta Metall Sin, 2011, 47(11): 1470-1476.
| [1] Versnyder F I, Shank M E. Mater Sci Eng, 1970; A6: 213[2] Chen J Y, Zhao B, Feng Q, Cao L M, Sun Z Q. Acta Metall Sin, 2010; 46: 897(陈晶阳, 赵宾, 冯 强, 曹腊梅, 孙祖庆. 金属学报, 2010; 46: 897)[3] Konter M, Kats E, Hofmann N A. In: Pollock T M, Kissinger R D, Bowman R R, Green K A, Mclean M, Olson S, Schirra J J eds., Superalloys 2000, Warrendale, PA: TMS, 2000: 189[4] Nakagawa Y G, Ohotomo Y, Saiga Y. In: Tien J K, Gell M, Maurer G, Wlodek S T eds., Superalloys 1980, Warrendale, PA: TMS, 1980: 267[5] Giamei A F, Tschinkel J G. Metall Trans, 1976; 7A: 1427[6] Fu H Z. Directional Solidification and Processing of Advanced Materials. Beijing: Science Press, 2008: 492(傅恒志. 先进材料定向凝固. 北京: 科学出版社, 2008: 492)[7] McLean M. Directionally Solidified Materials for High Temperature Service. UK: The Metals Society, 1983: 11[8] Chen H J, Wever H. J Mater Eng, 2000; 11: 45(陈鸿均, Wever H. 材料工程, 2000; 11: 45 )[9] Jiang L W, Li S S, Qiu Z C, Han Y F. Acta Metall Sin, 2009; 45: 547(蒋立武, 李树索, 邱自成, 韩亚芳. 金属学报, 2009; 45: 547)[10] Lamm M, Singer R F. Metall Mater Trans, 2007; 38A: 1177[11] Whitesell H S, Li L, Overfelt R A. Metall Mater Trans, 2000; 31B: 546[12] Zhang J, Li J G, Jin T, Sun X F, Hu Z Q. J Mater Sci Technol, 2010; 26: 889[13] Takao M, Toshiharu K, Yutaka K, Hiroshi H. Acta Mater, 2004; 52: 3737[14] Bhambri A K, Kattamis T Z, Morral J E. Matall Trans, 1975; 6B: 532[15] Zupaniˇc F, Bomˇcina T, Kriˇzman A, Markoli B, Spaic S. Scr Mater, 2002; 46: 667[16] Kearsy R M, Beddoes J C, Jaansalu K M, Thompson W T, Au P. In: Green K A, Pollock TM, Harada H, Howson T E, Reed R C, Schirra J J, Walston S eds., Superalloys 2004, Warrendale, PA: TMS, 2004: 723[17] Kuleshova E A, Cherkasova E R, Logunov A V. Metalloved Term Obrab Met, 1981; 6: 20[18] Guo X P, Fu H Z, Sun J H. Metall Mater Trans, 1997; 28A: 997[19] Liu L, Sommer F, Fu H Z. Scr Metall Mater, 1994; 30: 587[20] Zhao K, Ma Y X, Lou L H. J Alloys Compd, 2009; 475: 648[21] Elliott A J, Pollock T M, Tin S, King W T, Huang S C, Gigliotti M F. Metall Mater Trans, 2004; 35A: 3221[22] Zhang J, Lou L H. J Mater Sci Technol, 2007; 23: 289[23] G¨und¨uz M, C¸ad?rl? E. Mater Sci Eng, 2002; A327: 167[24] Hunt J D. Solidification and Casting of Metals. London: The Metal Society, 1979: 3[25] ZhangWG. PhD Thesis, Northwestern Polytechnical University, Xi’an, 2009(张卫国. 西北工业大学博士论文, 西安, 2009)[26] Min Z X, Shen J, Wang L S, Feng Z R, Liu L, Fu H Z. Acta Metall Sin, 2010; 46: 1075(闵志先, 沈军, 王灵水, 冯周荣, 刘林, 傅恒志. 金属学报, 2010; 46: 1075)[27] Zheng Y R. Acta Metall Sin, 1986; 22: 119(郑运荣. 金属学报, 1986; 22: 119)[28] Liu L. PhD Thesis, Xi’an: Northwestern Polytechnical University, 1988(刘林. 西北工业大学博士论文, 西安, 1988) |
|