热锻温度对TG6高温钛合金显微组织和力学性能的影响 |
王涛,郭鸿镇,张永强,姚泽坤,谭立军 |
西北工业大学材料科学与工程学院, 西安 710072 |
|
EFFECTS OF HOT FORGING TEMPERATURE ON MICROSTRUCTURE AND MECHANICAL PROPERTY OF TG6 HIGH TEMPERATURE TITANIUM ALLOY |
WANG Tao, GUO Hongzhen, ZHANG Yongqiang, YAO Zekun, TAN Lijun |
School of Materials Science and Engineering, Northwestern Polytechnical University, Xi’an 710072 |
引用本文:
王涛 郭鸿镇 张永强 姚泽坤 谭立军. 热锻温度对TG6高温钛合金显微组织和力学性能的影响[J]. 金属学报, 2010, 46(8): 913-920.
,
,
,
,
.
EFFECTS OF HOT FORGING TEMPERATURE ON MICROSTRUCTURE AND MECHANICAL PROPERTY OF TG6 HIGH TEMPERATURE TITANIUM ALLOY[J]. Acta Metall Sin, 2010, 46(8): 913-920.
[1] Bania P J. J Met, 1988; 3: 20
[2] Harry Chandler. Heat Treaters’s Guide: Practices and Procedures for Nonferrous Alloys. Ohio: ASM International, 1996: 511
[3] Tetyukhin V. In: Blenkinsop P A, Evans W J, Flower H M, es., Titanium’95: Science and Technoogy, Cambridge, UK: Cambridge University Press, 1996: 2430
[4] Cai J M, Li Z X, Ma J M, Huang X, Cao C X. Mater Rev, 2005; 19: 50
(蔡建明, 李臻熙, 马济民, 黄旭, 曹春晓. 材料导报, 2005; 19: 50)
[5] Zhang J, Li D. The 2 Phase In The High Temperature Titanium. Shenyang: Northeast University Press, 2002: 8
(张均, 李东. 高温钛合金中的α2相. 沈阳: 东北大学出版社, 2002: 8)
[6] Weiss I, Semiatin S L. Mater Sci Eng, 1998; A243: 46
[7] Sauer C, Luetjering G. J Mater Process Technol, 2001; 117: 311
[8] Guo H Z, Yao Z K, Feng C, Su Z W. Rare Met Mater Eng, 2003; 32: 566
(郭鸿镇, 姚泽坤, 冯 超, 苏祖武. 稀有金属材料与工程, 2003; 32: 566)
[9] Ma F C, Lu W J, Qin J N, Zhang D. Mater Sci Eng, 2006; A416: 59
[10] Zhang X Y, Zhao Y Q, Bai C G. Titanium Alloys and Application. Beijing: Chemical Industry Press, 2005: 177
(张喜燕, 赵永庆, 白晨光. 钛合金及应用. 北京: 化学工业出版社, 2005: 177)
[11] Zhou Y G, Zeng W D, Yu H Q. Mater Sci Eng, 2005; A393: 204
[12] Zhou Y G, Zeng W D, Yu H Q. Eng Sci, 2001; 3(5): 61
(周义刚, 曾卫东, 俞汉清. 中国工程科学, 2001; 3(5): 61)
[13] Yang Y, Xu F, Huang A J, Li G P. Acta Metall Sin, 2005; 41: 713
(杨义, 徐锋, 黄爱军, 李阁平. 金属学报, 2005; 41: 713)
[14] Wang X Y, Liu J R, Lei J F, Cao M Z, Liu Y Y. Acta Metall Sin, 2007; 43: 1129
(王晓燕, 刘建荣, 雷家峰, 曹名洲, 刘羽寅. 金属学报, 2007; 43:1129)
[15] Sun Z C, Yang H. Mater Sci Eng, 2009; A523: 184
[16] Kong F T, Chen Y Y, Li B H. Acta Metall Sin, 2008; 44: 815
(孔凡涛, 陈玉勇, 李宝辉. 金属学报, 2008; 44: 815)
[17] Terlinde G, Luetjering G. Metall Trans, 1982; 13A: 1283
[18] Duan R, Cai J M, Li Z X. J Aeronaut Mater, 2007; 27(3): 17
(段锐, 蔡建明, 李臻熙. 航空材料学报, 2007; 27(3): 17)
[19] Chu M Y, Hui S X, Zhang Z, Shen J Y. J Chin Electron Microsc Soc, 2004; 23: 168
(储茂友, 惠松骁, 张翥, 沈剑韵. 电子显微学报, 2004; 23: 168)
[20] Xu F, Li G P, Yang R. Acta Metall Sin, 2006; 42: 770
(徐锋, 李阁平, 杨锐. 金属学报, 2006; 42: 770)
[21] Cui Y X, Wang C L. Fractograph Analysis of Metal. Harbin: Harbin Institute of Technology Press, 1998: 39
(崔约贤, 王长利. 金属断口分析. 哈尔滨: 哈尔滨工业大学出版社, 1998: 39)
[22] Filip R, Kubiak K, ZiajaW, Sieniawski J. J Mater Process Technol, 2003; 133: 84 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|