| 长期热老化对铸造奥氏体不锈钢组织和性能的影响 |
| 李时磊,王艳丽,李树肖,王西涛 |
| 北京科技大学新金属材料国家重点实验室, 北京 100083 |
|
| EFFECT OF LONG TERM AGING ON THE MICROSTRUCTURE AND MECHANICAL PROPERTIES OF CAST AUSTENITIC STAINLESS STEELS |
| LI Shilei, WANG Yanli, LI Shuxiao, WANG Xitao |
| State Key Laboratory for Advanced Metals and Materials, University of Science and Technology Beijing, Beijing 100083 |
引用本文:
李时磊 王艳丽 李树肖 王西涛. 长期热老化对铸造奥氏体不锈钢组织和性能的影响[J]. 金属学报, 2010, 46(10): 1186-1191.
,
,
,
.
EFFECT OF LONG TERM AGING ON THE MICROSTRUCTURE AND MECHANICAL PROPERTIES OF CAST AUSTENITIC STAINLESS STEELS[J]. Acta Metall Sin, 2010, 46(10): 1186-1191.
| [1] Pumphrey P H, Akhurst K N. Mater Sci Tech-Lond, 1990; 6: 211
[2] Bonnet S, Bourgoin J, Champredonde J, Guttmann D, Guttmann M. Mater Sci Tech-Lond, 1990; 6: 221
[3] Hale G E, Garwood S J. Mater Sci Tech-Lond, 1990; 6: 230
[4] Miller M K, Bentley J. Mater Sci Tech-Lond, 1990; 6: 285
[5] Brown J E, Cerezo A, Godfrey T J, Hetherington M G, Smith G D W. Mater Sci Tech-Lond, 1990; 6: 293
[6] Auger P, Danoix F, Menand A, Bonnet S, Bourgoin J, Guttmann M. Mater Sci Tech-Lond, 1990; 6: 301
[7] Mathew M D, Lietzan L M, Murty K L, Shah V N. Mat Sci Eng A-Struct, 1999; 269: 186
[8] Kawaguchi S, Sakamoto N, Takano G, Matsuda F, Kikuchi Y, Mraz L. Nucl Eng Des, 1997; 174(3): 273
[9] Yamada T, Okano S, Kuwano H. J Nucl Mater, 2006; 350(1): 47
[10] Danoix F, Auger P, Blavette D. Microsc Microanal. 2004; 10(3): 349
[11] Wang Y L. PhD Thesis, University of Science and Technology Beijing, 2001.
(王艳丽. 北京科技大学博士论文, 2001)
[12] Bethmont M, Meyzaud Y, Soulat P. Int J Pres Ves Pip. 1996; 65(3): 211
[13] Chung H M, Leax T R. Mater Sci Tech-Lond, 1990; 6: 249
[14] Chung H M. . Int J Pres Ves Pip, 1992; 50(1-3): 179
[15] Vrinat M, Cozar R, Meyzaud Y. Scripta Mater, 1986; 20(8):1101
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|