| 半固态条件下球晶生长形态的稳定性 |
| 统雷雷; 林鑫; 赵力宁;黄卫东 |
| (西北工业大学凝固技术国家重点实验室; 西安 710072) |
|
| MORPHOLOGICAL STABILITY OF GLOBULAR CRYSTAL DURING SEMI--SOLID PROCESSING |
| TONG Leilei; LIN Xin; ZHAO Lining; HUANG Weidong |
| State Key Laboratory of Solidification Processing; Northwestern Polytechnical University; Xi'an 710072 |
引用本文:
统雷雷 林鑫 赵力宁 黄卫东. 半固态条件下球晶生长形态的稳定性[J]. 金属学报, 2009, 45(6): 737-743.
,
,
,
.
MORPHOLOGICAL STABILITY OF GLOBULAR CRYSTAL DURING SEMI--SOLID PROCESSING[J]. Acta Metall Sin, 2009, 45(6): 737-743.
| [1] Flemings M C. Metall Trans, 1991; 22B: 957
[2] Spencer D B, Mehrabian R, Flemings M C. Metall Trans,1972; 3A: 1925
[3] Doherty R D, Lee H I, Feest E A. Mater Sci Eng, 1984; 65: 181
[4] Hellawell A. In: Kirkwood D H, Kapranos P eds., Proc 4th Int Conf on Semi–Solid Processing of Alloys and Composites. Sheffield, UK: The University of Sheffield, 1996: 60
[5] Van Dam J C, Mischgofsky F H. J Mater Sci, 1982; 17: 989
[6] Fan Z. Int Mater Rev, 2002; 47: 49
[7] Li T, Lin X, Huang W D. Acta Mater, 2006; 54: 481
[8] Lin X, Li T, Huang W D. Solid State Phenom, 2006; 16–17: 155
[9] Li T, Huang W D, Lin X. Chin J Nonferrous Met, 2000; 10: 635
(李 涛, 黄卫东, 林 鑫. 中国有色金属学报, 2000; 10: 635)
[10] Ji S, Fan Z, Bevis M J. Mater Sci Eng, 2001; A299: 210
[11] Martinez R A, Flemings M C. Metall Mater Trans, 2005;36A: 2205
[12] James E S J, Donald O F, William F K. Scr Metall, 1984; 18: 677
[13] Trivedi R. J Cryst Growth, 1980; 48: 93
[14] Schulze T P, Davis S H. J Cryst Growth, 1995; 149: 253
[15] Turnbull D, Fisher J C. J Chem Phys,1949; 17: 71
[16] Liu Z E. Foundations of Materials Science. Xi’an: Northwestern Polytechnical University Press, 2000: 81
(刘智恩. 材料科学基础. 西安: 西北工业大学出版社, 2000: 81)
[17] Li T, Lin X, Wang L L, Xue L, Zhao X M, Huang W D.J Mater Sci Eng, 2003; 21: 741
(李涛, 林 鑫, 王琳琳, 薛蕾, 赵晓明, 黄卫东. 材料科学与工程学报, 2003; 21: 741)
[18] Iida T, Guthrie R I L. The Physical Properties of Liquid Metal. Oxford: Clarenpon Press, 1993: 173 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|