混沌对流下的半固态A356铝合金初生相形貌演变研究* |
刘政1(),张嘉艺2,罗浩林2,邓可月1 |
1 江西理工大学机电工程学院, 赣州 341000 2 江西理工大学材料科学与工程学院, 赣州 341000 |
|
RESEARCH ON MORPHOLOGY EVOLUTION OF PRIMARY PHASE IN SEMISOLID A356 ALLOY UNDER CHAOTIC ADVECTION |
Zheng LIU1(),Jiayi ZHANG2,Haolin LUO2,Keyue DENG1 |
1 School of Mechanical and Electronic Engineering, Jiangxi University of Science and Technology, Ganzhou 341000, China 2 School of Materials Science and Engineering, Jiangxi University of Science and Technology, Ganzhou 341000, China |
引用本文:
刘政,张嘉艺,罗浩林,邓可月. 混沌对流下的半固态A356铝合金初生相形貌演变研究*[J]. 金属学报, 2016, 52(2): 177-183.
Zheng LIU,
Jiayi ZHANG,
Haolin LUO,
Keyue DENG.
RESEARCH ON MORPHOLOGY EVOLUTION OF PRIMARY PHASE IN SEMISOLID A356 ALLOY UNDER CHAOTIC ADVECTION[J]. Acta Metall Sin, 2016, 52(2): 177-183.
[1] | Lin X, Tong L L, Zhao L N, Wang L N, Wang M, Huang W D.Trans Nonferrous Met Soc China, 2010; 20: 826 | [2] | Zhao L N, Lin X, Huang W D.Acta Metall Sin, 2011; 47: 403 | [2] | (赵力宁, 林鑫, 黄卫东. 金属学报, 2011; 47: 403) | [3] | Xu J F, Wei B B.Acta Phys Sin, 2004; 53: 1909 | [3] | (徐锦峰, 魏炳波. 物理学报, 2004; 53: 1909) | [4] | Nikrityuk P A, Eckert K, Grundmann R.Int J Heat Mass Trans, 2006; 49: 1501 | [5] | Nikrityuk P A, Ungarish M, Eckert K, Grundmann R.Phys Fluids, 2005; 17: 101 | [6] | Pan Y, Zhang C Y.Acta Metall Sin, 2001; 37: 1035 | [6] | (潘冶, 张春燕. 金属学报, 2001; 37: 1035) | [7] | Campanella T, Charbon C, Rappaz M.Metall Mater Trans, 2004; 35A: 3201 | [8] | Zhao J Z, Li H L, Zhao L.Acta Metall Sin, 2009; 45: 1435 | [8] | (赵九洲, 李海丽, 赵雷. 金属学报, 2009; 45: 1435) | [9] | Gao S Y, Le Q C, Zhang Z Q, Cui J Z.Bull Mater Sci, 2012; 35: 651 | [10] | Eckert S, Nikrityuk P A, Willers B, Räbiger D, Shevchenko N, Neumann H H.Eur Phys J Spec Topics, 2013; 220: 123 | [11] | Poole G M, Heyen M, Nastac L, El-Kaddah N.Metall Mater Trans, 2014; 45B: 1834 | [12] | Aref H.J Fluid Mech, 1984; 143: 21 | [13] | Arratic P E, Muzzio F J.Ind End Chem Res, 2004; 43: 6557 | [14] | Bresler L, Shinbrot T, Metcalfe G, Ottino J M.Chem Eng Sci, 1997; 52: 1623 | [15] | Lu G M, Zhao D Z, Wang P, Cui J Z.J Northeastern Univ (Nat Sci), 2007; 28: 353 | [15] | (路贵民, 赵大志, 王平, 崔建忠. 东北大学学报(自然科学版), 2007; 28: 353) | [16] | Tao W Y, Zhao S D, Lin W J.J Mech Eng, 2012; 48(14): 50 | [16] | (陶文毓, 赵升吨, 林文捷. 机械工程学报, 2012; 48(14): 50) | [17] | Sun K H, He S B, He Y, Yin L Z.Acta Phys Sin, 2013; 62: 1 | [17] | (孙克辉, 贺少波, 何毅, 尹林子. 物理学报, 2013; 62: 1) | [18] | Zhu Y Z, Yi S H, Kong X P.Acta Phys Sin, 2015; 64: 701 | [18] | (朱杨柱, 易仕和, 孔小平. 物理学报, 2015; 64: 701) | [19] | Zheng G B, Jin N D.Acta Phys Sin, 2009; 58: 4485 | [19] | (郑桂波, 金宁德. 物理学报, 2009; 58: 4485) | [20] | Schouten J C, Takens F, van den Bleek C M.Phys Rev, 1994; 49E: 126 | [21] | Wang Z F, Wang Z H.Chin J Comput, 2012; 35: 364 | [21] | (王中锋, 王志海. 计算机学报, 2012; 35: 364) | [22] | Falconer K J.Math Proc Camb Phil Soc, 1988; 103: 339 | [23] | Li S G.Fractals. Beijing: Higher Education Press, 2004: 55 | [23] | (李水根. 分形. 北京:高等教育出版社, 2004: 55) | [24] | Liu Z H, Sun R X, Wang Y D.Ciesc J, 2014; 65: 3340 | [25] | Fan Z, Chen J Y.Mater Sci Technol, 2002; 18: 258 | [26] | Liu F F, Yang C J, Su Q, Wang D H, Zhang Y Z.J Mech Eng, 2010; 46(19): 24 | [27] | Yang X W, Zhu J C, He D.Trans Nonferrous Met Soc China, 2013; 23: 1442 |
|
|