| 激光立体成形Ti60--Ti2AlNb梯度材料的组织与相演变 |
| 杨模聪; 林 鑫;许小静;陈 静; 黄卫东 |
| (西北工业大学凝固技术国家重点实验室; 西安 710072) |
|
| MICROSTRUCTURE AND PHASE EVOLUTION IN Ti60--Ti2AlNb GRADIENT MATERIAL PREPARED BY LASER SOLID FORMING |
| YANG Mocong; LIN Xin; XU Xiaojing; CHEN Jing; HUANG Weidong |
| State Key Laboratory of Solidification Processing; Northwestern Polytechnical University; Xi'an 710072 |
引用本文:
杨模聪 林鑫 许小静 陈静 黄卫东. 激光立体成形Ti60--Ti2AlNb梯度材料的组织与相演变[J]. 金属学报, 2009, 45(6): 729-736.
,
,
,
,
.
MICROSTRUCTURE AND PHASE EVOLUTION IN Ti60--Ti2AlNb GRADIENT MATERIAL PREPARED BY LASER SOLID FORMING[J]. Acta Metall Sin, 2009, 45(6): 729-736.
| [1] Cao C X. Rare Met Lett, 2006; 25(1): 17
(曹春晓. 稀有金属快报, 2006; 25(1): 17)
[2] Tang Z L, Wang F H, Wu W T, Wang Q J, Li D. Mater Sci Eng, 1998; A255: 133
[3] Wanjara P, Jahazi M, Monajati H, Yue S. Mater Sci Eng, 2006; A416: 300
[4] Vermaa R, Ghosh A K, Merrickb H, Mukherji T. Mater Sci Eng, 1995; A191: 151
[5] Tetyukhin V, Levin I, Ilyenko V. Heatresistant Ttitanium Alloys with Enhanced, Heat Resistance, Thermal Stability. Cambridge, UK: Cambridge University Press, 1996:2430
[6] Li M Q, Lin Y Y. Int J Hydrogen Energy, 2007; 32: 626
[7] Cai J M, Li Z X, Ma J M, Huang X, Cao C X. Mater Rev,2005; 19(1): 50
(蔡建明, 李臻熙, 马济民, 黄旭, 曹春晓. 材料导报, 2005; 19(1): 50)
[8] Banerjee D, Gogia A K, Nandy T K, Joshi V A. Acta Metall, 1988; 36: 871
[9] Banerjee D. Prog Mater Sci, 1997; 42: 135
[10] Huang W D, Lin X, Chen J, Liu Z X, Li Y M. Laser Solid Forming. Xi’an: Northwestern Polytechnical University Press, 2007: 5
(黄卫东, 林鑫, 陈静, 刘振侠, 李延民. 激光立体成形. 西安: 西北工业大学出版社, 2007: 5)
[11] Lin X, Yue T M, Yang H O, Huang W D. Acta Mater, 2006; 54: 1901
[12] Lin X, Yue T M, Yang H O, Huang W D. Mater Sci Eng, 2005; A391: 325
[13] Liu J T, Lin X, L¨u X W, Chen J, Huang W D. Acta Metall Sin, 2008; 44: 1006
(刘建涛, 林鑫, 吕晓卫, 陈静, 黄卫东. 金属学报, 2008; 44: 1006)
[14] Xu X J, Lin X, Yang M C, Chen J, Huang W D. Acta Metal Sin, 2008; 44: 1013
(许小静, 林鑫, 杨模聪, 陈静, 黄卫东. 金属学报, 2008; 44: 1013)
[15] Collins P C, Banerjee R, Banerjee S, Fraser H L. Mater Sci Eng, 2003; A352: 118
[16] Deng A H. Shanghai Nonferrous Met, 1999; 20: 193
(邓安华. 上海有色金属, 1999; 20: 193)
[17] Wang J Y, Ge Z M, Zhou Y B. Aeronautical Titanium Alloy. Shanghai: Shanghai Science & Technology Press, 1985: 120
(王金友, 葛志明, 周彦邦. 航空用钛合金. 上海: 上海科学技术出版社, 1985: 120)
[18] Zhang J, Ma H F. J Shenyang Univ, 2006; 18(4): 1
(张钧, 马鸿峰. 沈阳大学学报, 2006; 18(4): 1)
[19] Boehlert C J, Majumdar B S, Seetharaman V, Miracle D B. Metall Mater Trans, 1999; 30A: 2305 |
|
Viewed |
|
|
|