Please wait a minute...
金属学报  2009, Vol. 45 Issue (4): 460-463    
  论文 本期目录 | 过刊浏览 |
Co1-xNixFe2O4/SiO2纳米复合材料的磁性
华杰1;刘梅2;冯明1;2;徐仕翀1;2;尹基哲1;李海波1
1. 吉林师范大学凝聚态物理与材料科学研究所; 四平 136000
2. 哈尔滨工业大学材料科学与工程学院; 哈尔滨 150001
MAGNETIC PROPERTIES OF Co1-xNixFe2O4/SiO2  NANOCOMPOSITES
HUA Jie 1; LIU Mei 1; FENG Ming 1;2; XU Shichong 1;2; YIN Jizhe 1; LI Haibo 1
1. Institute of Condensed Matter Physics and Material Science; Jilin Normal University; Siping 136000
2. School of Materials Science and Engineering; Harbin Institute of Technology; Harbin 150001
引用本文:

华杰 刘梅 冯明 徐仕翀 尹基哲 李海波. Co1-xNixFe2O4/SiO2纳米复合材料的磁性[J]. 金属学报, 2009, 45(4): 460-463.
, , , , , . MAGNETIC PROPERTIES OF Co1-xNixFe2O4/SiO2  NANOCOMPOSITES[J]. Acta Metall Sin, 2009, 45(4): 460-463.

全文: PDF(1758 KB)  
摘要: 

采用溶胶--凝胶法制备了Co1-xNixFe2O4/SiO2(0 ≤x ≤1.0)纳米复合材料. 利用XRD, TEM, 振动样品磁强计(VSM)和Mossbauer谱测试了900℃热处理样
品的结构、晶粒尺寸和磁性. 结果表明, 样品中Co1-xNixFe2O4铁氧体的平均晶粒尺寸在15---20 nm之间, Ni2+的掺杂引起CoFe2O4晶胞体积减小. VSM结果表明, 随Ni2+含量的增加, 样品的比饱和磁化强度和矫顽力变小. Mossbauer谱表明, 室温下各样品均处于磁有序状态, 样品的内磁场随Ni2+含量的增加而变小.

关键词 : 铁氧体,  纳米复合材料,  结构,  磁性,  Mossbauer谱    
Abstract:

Nanocomposites Co1-xNixFe2O4/SiO2   were prepared by sol–gel method using tetraethyl orthosilicate and nitrates, in which SiO2 is used to restrict the growth of ferrite crystalline and remove the agglomeration. XRD and TEM are used to characterize structures and morphologies. The composites sintered at 900 ℃consist of spinel phase with size ranging from 15 to 20 nm and amorphous SiO2. The doping of Ni2+ reduces the volume of unit cell of the spinel phase. The magnetic properties of the Co1-xNixFe2O4/SiO2   nanocomposites were measured by vibrating sample magnetometer and Mossbauer spectroscopy. The results indicate that the saturation magnetization decreases from 41.8 A·m2/kg to 23.0 A·m2/kg with increasing Ni2+ content. At the same time the coercivity decreases from 104.2 kA/m to 5.4 kA/m, which may originate from the variation of anisotropy induced by Co2+ ions in octahedral sites. All the samples are magnetic order state, the hyperfine magnetic field of the nanocomposites decreases with increasing Ni2+ content.

Key words: ferrite;nanocomposite;structure;magnetic property;Mössbauer effect
收稿日期: 2008-09-18     
ZTFLH: 

O482.5

 
基金资助:

吉林省科技发展计划基金资助项目20060803

作者简介: 华杰, 女, 1973年生, 讲师

[1] Plocek J, Hutlov´a A, Niznansky D, Bursik J, Rehspringer J -L, Micka Z. J Non-Cryst Solids, 2003; 315: 70
[2] Garcia–Cerda L A, Torres–Garcia V A, Matutes–Aquino J A, Ayala–Valenzuela O E. J Alloys Compd, 2004; 369: 148
[3] Liu X M, Fu S Y, Huang C J. J Magn Magn Mater, 2004; 281: 234
[4] Zhang S P, Dong D W, Sui Y, Liu Z G, Wang H X, Qian Z N, Su W H. J Alloys Compd, 2006; 415: 257
[5] Yan C H, Xu Z G, Cheng F X, Wang Z M, Sun L D, Liao C S, Jia J T. Solid State Commun, 1999; 111: 287
[6] Li S C, Vijay T J, O’Connor C, Harris V, Carpenter E. J Appl Phys, 2000; 87: 6223
[7] Wang Y C, Ding J, Yin J H, Liu H, Yi J B, Yu S. J Appl Phys, 2005; 98: 4306
[8] Gui L, Zhong Y B, Fu X M, Lei Z S, Ren Z M. Acta Metall Sin, 2007; 43: 529
(桂 林, 钟云波, 傅小明, 雷作胜, 任忠鸣. 金属学报, 2007;  43: 529)
[9] El–Sayed H M. J Alloys Compd, (2008), doi: 10.1016/j. jallcom. 2008. 06. 139
[10] Zhao L J, Yang H, Zhao X P, Yu L X, Cui Y M, Feng S H. Mater Lett, 2006; 60: 1
[11] Chae K P, Lee J G, Kweon H S, Lee Y B. J Magn Magn Mater, 2004; 283: 103
[12] Arulmurugan R, Vaidyanathan G, Sendhilnathan S, Jeyadevan B. J Magn Magn Mater, 2006; 303: 131
[13] Niu Z P, Wang Y, Li F S. J Mater Sci, 2006; 41: 5726
[14] Gul I H, Amin F, Abbasi A Z, Anis–ur–Rehman M, Maqsood A. Scr Mater, 2007; 56: 497
[15] Mathe V L, Kamble R B. Mater Res Bull, 2008; 43: 2160
[16] Li H B, Chen J Y, Liu M, Feng M, Hua J. Chem Res Chin Univ, 2007; 28: 614
(李海波, 陈敬艳, 刘 梅, 冯 明, 华 杰. 高等化学学报, 2007; 28: 614)
[17] Zhang B J, Chen J Y, Liu M, Meng X D, Hua J, Li H B. Acta Mater Comp Sin, 2008; 25(3): 144
(张伯军, 陈敬艳, 刘 梅, 孟祥东, 华 杰, 李海波. 复合材料学报, 2008; 25(3): 144)
[18] Du Y W. Ferrite. Nanjing: Phoenix Science Press, 1996:62
(都有为. 铁氧体. 南京: 江苏科学技术出版社, 1996: 62)
[19] Ma R Z, Xu Y T. Mossbauer Spectroscopy. Beijing: Science Press, 1996: 351
(马如璋, 徐英庭. 穆斯堡尔谱学. 北京: 科学出版社, 1996: 351)

[1] 袁江淮, 王振玉, 马冠水, 周广学, 程晓英, 汪爱英. Cr2AlC涂层相结构演变对力学性能的影响[J]. 金属学报, 2023, 59(7): 961-968.
[2] 李谦, 刘凯, 赵天亮. 弹性拉应力下Q235碳钢在5%NaCl盐雾中的成锈行为及其机理[J]. 金属学报, 2023, 59(6): 829-840.
[3] 张德印, 郝旭, 贾宝瑞, 吴昊阳, 秦明礼, 曲选辉. Y2O3 含量对燃烧合成Fe-Y2O3 纳米复合粉末性能的影响[J]. 金属学报, 2023, 59(6): 757-766.
[4] 王寒玉, 李彩, 赵璨, 曾涛, 王祖敏, 黄远. 基于纳米活性结构的不互溶W-Cu体系直接合金化及其热力学机制[J]. 金属学报, 2023, 59(5): 679-692.
[5] 刘满平, 薛周磊, 彭振, 陈昱林, 丁立鹏, 贾志宏. 后时效对超细晶6061铝合金微观结构与力学性能的影响[J]. 金属学报, 2023, 59(5): 657-667.
[6] 邵晓宏, 彭珍珍, 靳千千, 马秀良. 镁合金LPSO/SFs结构间{101¯2}孪晶交汇机制的原子尺度研究[J]. 金属学报, 2023, 59(4): 556-566.
[7] 李谦, 孙璇, 罗群, 刘斌, 吴成章, 潘复生. 镁基材料中储氢相及其界面与储氢性能的调控[J]. 金属学报, 2023, 59(3): 349-370.
[8] 刘来娣, 丁彪, 任维丽, 钟云波, 王晖, 王秋良. DZ445镍基高温合金高温长时间氧化形成的多层膜结构[J]. 金属学报, 2023, 59(3): 387-398.
[9] 刘路军, 刘政, 刘仁辉, 刘永. Nd90Al10 晶界调控对晶界扩散磁体磁性能和微观结构的影响[J]. 金属学报, 2023, 59(11): 1457-1465.
[10] 高晗, 刘力, 周笑宇, 周心怡, 蔡汶君, 周泓伶. Ti6Al4V表面微纳结构的制备及生物活性[J]. 金属学报, 2023, 59(11): 1466-1474.
[11] 杨超, 卢海洲, 马宏伟, 蔡潍锶. 选区激光熔化NiTi形状记忆合金研究进展[J]. 金属学报, 2023, 59(1): 55-74.
[12] 韩冬, 张炎杰, 李小武. 短程有序对高层错能Cu-Mn合金拉-拉疲劳变形行为及损伤机制的影响[J]. 金属学报, 2022, 58(9): 1208-1220.
[13] 刘志愿, 王永贵, 赵成玉, 杨婷, 夏爱林. p型方钴矿热电材料纳米-介观尺度微结构调控[J]. 金属学报, 2022, 58(8): 979-991.
[14] 解磊鹏, 孙文瑶, 陈明辉, 王金龙, 王福会. 制备工艺对FGH4097高温合金微观组织与性能的影响[J]. 金属学报, 2022, 58(8): 992-1002.
[15] 谷瑞成, 张健, 张明阳, 刘艳艳, 王绍钢, 焦大, 刘增乾, 张哲峰. 三维互穿结构SiC晶须骨架增强镁基复合材料制备及其力学性能[J]. 金属学报, 2022, 58(7): 857-867.