| 陶瓷壳型面层材料与Ti46Al1B阀门铸件的界面反应 |
| 马颖澈;王玮东;陈波; 高明;刘奎;李依依 |
| 中国科学院金属研究所; 沈阳 110016 |
|
| INTERFACE REACTION BETWEEN CERAMIC MOULDS AND Ti46Al1B AS--CAST VALVES |
| MA Yingche; WANG Weidong; CHEN Bo; GAO Ming; LIU Kui; LI Yiyi |
| Institute of Metal Research; Chinese Academy of Sciences; Shenyang 110016 |
引用本文:
马颖澈 王玮东 陈波 高明 刘奎 李依依. 陶瓷壳型面层材料与Ti46Al1B阀门铸件的界面反应[J]. 金属学报, 2009, 45(3): 369-373.
,
,
,
,
,
.
INTERFACE REACTION BETWEEN CERAMIC MOULDS AND Ti46Al1B AS--CAST VALVES[J]. Acta Metall Sin, 2009, 45(3): 369-373.
| [1] Kim Y W. Mater Sci Eng, 1995; A192–193: 519
[2] Kim Y W. Acta Metall, 1999; 12: 334
[3] LorettoMH, HorspoolD, Botten R, HuD, Li Y G, Srivastava D, Sharman R, Wu X. Mater Sci Eng, 2002; A329–331: 1
[4] Yamaguchi M, Inui H. In: Daloria R, Lewwandowski J J, Liu C T, Martin P L, Miracle D B, Nathal M V, eds., Structural Intermetallics, Warrendale: TMS, 1993: 127
[5] Lapin J, Nazmy M. Mater Sci Eng, 2004; A380: 298
[6] Klaus G. Intermetallics, 2006; 14: 355
[7] Liu K, Ma Y C, Gao M, Rao G B, Li Y Y, Wei K, Wu X H, Loretto M H. Intermetallics, 2005; 13: 925
[8] Blum M, Jarczyk G, Scholz H, Pleier S, Busse P, Laudenberg H J, Segtrop K, Simon R. Mater Sci Eng, 2002; A329–331: 616
[9] Sommer A W, Keijzers G C. In: Kim Y W, Clemens H, Rosenberger A H, eds., Gamma Titanium Aluminides, Warrendale: TMS, 2003: 3
[10] Jia Q, Cui Y Y, Yang R. Acta Metall Sin, 2002; 38: 351
(贾清, 崔玉友, 杨锐. 金属学报, 2002; 38: 351)
[11] Jia Q, Cui Y Y, Yang R. J Mater Sci, 2006; 41: 3045
[12] Jones S, Bentley S A, Marquis P M. Br Ceram Trans, 2002; 101: 100
[13] Nan H, Xie C M. Acta Metall Sin, 2002; 38: 345
(南海, 谢成木. 金属学报, 2002; 38: 345)
[14] Yan C F, Zhao G J, Hang Y, Xu J. J Synth Cryst, 2005; 34: 144
(严成锋, 赵广军, 杭寅, 徐军. 人工晶体学报, 2005; 34: 144)
[15] Kobayashi Y, Tsukihashi F. High Temp Mater Processes, 2000; 19: 211 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|