Please wait a minute...
金属学报  2009, Vol. 45 Issue (3): 374-377    
  论文 本期目录 | 过刊浏览 |
Zr55Cu30Al12Ni3非晶超薄箔材的快速凝固焊接
翟秋亚;徐锦锋; 张兴;杨金山;郭学锋
西安理工大学材料学院; 西安 710048
RAPID SOLIDIFICATION WELDING OF ULTRA--THIN Zr55Cu50Al12Ni3 AMORPHOUS FOILS
ZHAI Qiuya; XU Jinfeng; ZHANG Xing; YANG Jinshan; GUO Xuefeng
School of Materials Science and Engineering; Xi'an University of Technology; Xi'an 710048
引用本文:

翟秋亚 徐锦锋 张兴 杨金山 郭学锋. Zr55Cu30Al12Ni3非晶超薄箔材的快速凝固焊接[J]. 金属学报, 2009, 45(3): 374-377.
. RAPID SOLIDIFICATION WELDING OF ULTRA--THIN Zr55Cu50Al12Ni3 AMORPHOUS FOILS[J]. Acta Metall Sin, 2009, 45(3): 374-377.

全文: PDF(869 KB)  
摘要: 

应用微型储能焊机实现了厚度为25---35 μm的Zr55Cu30Al12Ni3非晶箔材的快速凝固连接. XRD测试表明, 接头仍为非晶结构. 计算的接头冷却速率高达106 K/s, 远大于形成锆基非晶合金的临界冷却速率, 有效地抑制了接头区的晶化. 接头尺寸微小, 直径为60---90 μm, 未产生气孔、夹杂等焊接缺陷. 接头剪切强度高达1141 MPa. 高的电阻率特性使非晶合金的焊接能量明显低于晶态合金.

关键词 : 锆基非晶合金,  超薄箔,  快速凝固焊接,  接头性能    
Abstract:

The rapid solidification welding of Zr55Cu30Al12Ni3 amorphous foils with the thickness of 25---35 μm was conducted using a micro--type capacitor discharge welder. XRD analysis shows that the joint presents still amorphous structure under the rapid solidification welding conditions. The joint cooling rate calculated is high up to 106 K/s, which is much higher than that of critical cooling rate of amorphous Zr base alloy, and effectively suppresses the crystallization of joint zone. The micro joints with the size of 60---90 μm in diameter are produced and there are no welding defects such as porosity and inclusions within the joints. The joint shear strength is up to 1141 MPa. Contributing to higher electrical resistivity, the welding energy for welding metal glass foils is lower than that of crystallized metal foils remarkably.

Key words: Zr base amorphous alloy    ultra--thin foil    rapid solidification welding    mechanical property of joint
收稿日期: 2008-08-18     
ZTFLH: 

TG139.8

 
基金资助:

陕西省自然科学基金项目2006E134, 2006E120和陕西省教育厅科学研究计划项目06JK220资助

作者简介: 翟秋亚, 1963年生, 副教授, 博士

[1] Shoji T, Kawamura Y, Ohno Y}Mater Sci Eng, 2004; A375–377: 394
[2] Kagao S, Kawamura Y, Ohno Y}Mater Sci Eng, 2004; A375–377: 312
[3] Kawamura Y}Mater Sci Eng, 2004; A375–377: 112
[4] Swiston A J, Hufnagel T C, Weihs T P. Scr Mater, 2003; 48: 1575
[5] Zhai Q Y, Xu J F}Acta Metall Sin, 2005; 41: 755
(翟秋亚, 徐锦锋. 金属学报, 2005; 41: 755)

[6] Xu J F, Zhai Q Y, Yuan S. J Mater Sci Technol, 2004; 20: 431
[7] Lu Z P, Liu C T. Phys Rev Lett, 2003; 91: 115501
[8] Xu M, Sun Y, Quan M X, Wang Y D, Zuo L. Acta Metall Sin, 2007; 43: 699
(徐民, 孙 羽, 全明秀, 王沿东, 左良. 金属学报, 2007; 43: 699)

[9] Zhai Q Y, Zhang X, Xu J F. Trans China Weld Inst, 2007; 28(9): 99
(翟秋亚, 张兴, 徐锦锋. 焊接学报, 2007; 28(9): 99)

[10] Brandes E A. Smithells Metals Reference Book. 6th Ed., London: Butterworth & Co (Publishers) Ltd., 1983: 14

[1] 马宗义, 商乔, 倪丁瑞, 肖伯律. 镁合金搅拌摩擦焊接的研究现状与展望[J]. 金属学报, 2018, 54(11): 1597-1617.
[2] 雷奕; 黑祖昆; Mohique; Calvo-Dahlborg; Jean-Marie; Dubois; DONG; Chuang . Zr-二十面体准晶-十次准晶伪三元系中非晶的形成[J]. 金属学报, 2003, 39(6): 573-578 .
[3] 王晓东; 齐民; 董闯 . 铝元素的添加对锆基合金非晶形成能力影响的电子结构模型[J]. 金属学报, 2002, 38(12): 1241-1245 .