| 微/纳米Cu-W粉末激光烧结体的显微组织 |
| 顾冬冬;沈以赴 |
| 南京航空航天大学材料科学与技术学院; 南京 210016 |
|
| MICROSTRUCTURES OF LASER SINTERED MICRON/ NANO-SIZED Cu-W POWDER |
| GU Dongdong;SHEN Yifu |
| College of Materials Science and Technology; Nanjing University of Aeronautics and Astronautics; Nanjing 210016 |
引用本文:
顾冬冬 沈以赴. 微/纳米Cu-W粉末激光烧结体的显微组织[J]. 金属学报, 2009, 45(1): 113-118.
,
.
MICROSTRUCTURES OF LASER SINTERED MICRON/ NANO-SIZED Cu-W POWDER[J]. Acta Metall Sin, 2009, 45(1): 113-118.
| [1] Guo G C. Liquid Phase Sintering Powder Metallurgy Materials. Beijing: Chemical Industry Press, 2003: 97
(郭庚辰. 液相烧结粉末冶金材料. 北京: 化学工业出版社, 2003: 97)
[2] Fan J L, Huang B Y, Wang D L, Qu X H, Zhang C F. Rare Met Mater Eng, 2001; 30: 401
(范景莲, 黄伯云, 汪登龙, 曲选辉, 张传福. 稀有金属材料与工程, 2001; 30: 401)
[3] Liu B B, Lu Y N, Xie J X. Chin J Nonferrous Met, 2007; 17: 1410
(刘彬彬, 鲁岩娜, 谢建新. 中国有色金属学报, 2007; 17: 1410)
[4] Zhou Z J, Ge C C, Li J T. Acta Metall Sin, 2000; 36: 655
(周张健, 葛昌纯, 李江涛. 金属学报, 2000; 36: 655)
[5] da Costa F A, da Silva A G P, Gomes U U. Powder Technol, 2003; 134: 123
[6] Johnson J L, Brezovsky J J, German R M. Metall Mater Trans, 2005; 36A: 1557
[7] Johnson J L, Brezovsky J J, German R M. Metall Mater Trans, 2005; 36A: 2807
[8] Hong S H, Kim B K. Mater Lett, 2003; 57: 2761
[9] Yoon E S, Lee J S, Oh S T, Kim B K. Int J Refract Met Hard Mater, 2002; 20: 201
[10] Gu D D, Shen Y F, Fang S Q, Xiao J. J Alloys Compd, 2007; 438: 184
[11] Liu J H, Shi Y S, Lu Z L, Huang S H. Appl Phys, 2007;89A: 743
[12] Lin X, Yang H O, Chen J, Huang W D. Acta Metall Sin, 2006; 42: 361
(林鑫, 杨海欧, 陈静, 黄卫东. 金属学报, 2006; 42: 361)
[13] Yan M, Zhang S Q, Wang H M. Acta Metall Sin, 2007; 43: 472
(颜敏, 张述泉, 王华明. 金属学报, 2007; 43: 472)
[14] Dong C, Zhang S Q, Li A, Wang H M. Acta Metall Sin, 2008; 44: 598
(董翠, 张述泉, 李安, 王华明. 金属学报, 2008; 44: 598)
[15] Williams J M, Adewunmi A, Schek R M, Flanagan C L, Krebsbach P H, Feinberg S E, Hollister S J, Das S. Biomaterials, 2005; 26: 4817
[16] Kim D G, Lee B H, Oh S T, Kim Y D, Kang S G. Mater Sci Eng, 2005; A395: 333
[17] Hong S H, Kim B K, Munir Z A. Mater Sci Eng, 2005; A405: 325
[18] Yang M C, Song Z Z, Lu K. Acta Metall Sin, 2004; 40: 639
(杨明川, 宋贞祯, 卢柯. 金属学报, 2004; 43: 639)
[19] Gu D D, Shen Y F. Acta Metall Sin, 2007; 40: 968
(顾冬冬, 沈以赴. 金属学报, 2007; 43: 968)
[20] Simchi A, Pohl H. Mater Sci Eng, 2003; A359: 119
[21] Gu D D, Shen Y F. Metall Mater Trans, 2006; 37B: 967
[22] Arafune K, Hirata A. J Cryst Growth, 1999; 197: 811
[23] Teng X Y, Min G H, Liu H L, Shi Z Q, Wang H R, Ye Y F. Mater Sci Technol, 2001; 9: 383
(滕新营, 闵光辉, 刘含莲, 石志强, 王焕荣, 叶以富. 材料科学与工艺, 2001; 9: 383)
[24] Yuan Z F, Ke J J, Li J. Surface Tension of Metals and Alloys. Beijing: Science Press, 2006: 29
(袁章福, 柯家骏, 李晶. 金属及合金的表面张力. 北京: 科学出版社, 2006: 29)
[25] Shi L K, Gao S Y, Xi M Z, Ji H Z, Zhang Y Z, Du B L. Acta Metall Sin, 2006; 42: 449
(石力开, 高士友, 席明哲, 纪宏志, 张永忠, 杜宝亮. 金属学报, 2006; 42: 449)
[26] Anestiev L A, Froyen L. J Appl Phys, 1999; 86: 4008
[27] Niu H J, Chang I T H. Scr Mater, 1999; 41: 25
[28] Fischer P, Romano V, Weber H P, Karapatis N P, Boillat E, Glardon R. Acta Mater, 2003; 51: 1651
[29] The Chinese Society for Metals, The Nonferrous Metals Society of China. Handbook of Physical Properties of Metal Materials, Vol.1: Physical Properties of Metals and Testing Methods. Beijing: Metallurgical Industry Press, 1987: 323
(中国金属学会, 中国有色金属学会. 金属材料物理性能手册 (第1册: 金属物理性能及测试方法). 北京: 冶金工业
出版社, 1987: 323)
[30] Yang S M, Tao W Q. Heat Transfer. 3rd Ed., Beijing: Higher Education Press, 1998: 424
(杨世铭, 陶文铨. 传热学. 第3版, 北京: 高等教育出版社, 1998: 424)
[31] Chatterjee A N, Kumar S, Saha P, Mishra P K, Choudhury A R. J Mater Process Technol, 2003; 136: 151
[32] Yin H B, Emi T. Metall Mater Trans, 2003; 34B: 483 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|