| 热处理对AZ80镁合金结构及性能的影响 |
| 唐 伟; 韩恩厚; 徐永波;刘 路 |
| 中国科学院金属研究所材料环境腐蚀中心 |
|
| Effect of heat treatment on microstructure and properties of AZ80 magnesium alloy |
| TANG Wei; HAN Enhou; XU Yongbo; LIU Lu |
| Environmental Corrosion Center; Institute of Metal Research; The Chinese Academy of Sciences |
引用本文:
唐伟; 韩恩厚; 徐永波; 刘路 . 热处理对AZ80镁合金结构及性能的影响[J]. 金属学报, 2005, 41(11): 1199-1206 .
,
,
,
.
Effect of heat treatment on microstructure and properties of AZ80 magnesium alloy[J]. Acta Metall Sin, 2005, 41(11): 1199-1206 .
[1] Kojima Y, Aizawa T. Mater Sci Forum, 2003: 419-422: 3 [2] Schumann S, Friedrich H. Mater Sci Forum, 2003; 419- 422: 51 [3] Clark J B. Acta Metall, 1968; 16: 141 [4] Crawley A F, Milliken K S. Acta Metall, 1974; 22: 557 [5] Clawley A F, Lagowski B. Metall Trans, 1974; 5: 949 [6] Xiao X L, Luo C P, Nie J F, Muddle B C. Acta Metall Sin, 2001; 37:1 (肖晓玲,罗承萍.聂建峰,Muddle B C.金属学报,2001; 37:1) [7] Luo C P, Xiao X L, Liu J W, Nie J F, Muddle B C. Acta Metall Sin, 2002; 38: 709 (罗承萍,肖晓玲,刘江文,聂建峰,Muddle B C.金属学报, 2002;38:709) [8] Duly D, Zhang W Z, Audier M. Philos Mag, 1995; 71A: 187 [9] Celotto S. Acta Mater, 2000; 48: 1775 [10] Duly D, Cheynet M C, Brechet Y. Acta Metall Mater, 1994; 42: 3843 [11] Duly D, Cheynet M C, Brechet Y. Acta Metall Mater, 1994; 42: 3855 [12] Duly D, Brechet Y. Acta Metall Mater, 1994; 42: 3035 [13] Duly D, Brechet Y. Acta Metall Mater, 1992; 40: 2289 [14] Hillert M. Acta Metall, 1982; 30: 1689 [15] Duly D, Simon J P. Acta Metall Mater, 1995; 43: 101 [16] Na Y G, Yim C D. Mater Sci Forum, 2003; 419-422: 285 [17] Dahmen O. Acta Metall, 1982; 30: 63 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|