| GH742合金热变形行为与微观组织演化 |
| 张北江; 赵光普; 胥国华; 冯 涤 |
| 钢铁研究总院高温材料研究所 |
|
| Hot deformation behavior and micro-structure evolution of superalloy GH742 |
| ZHANG Beijiang; ZHAO Guangpu; XU Guohua; FENG Di |
| High Temperature Materials Division; Central Iron and Steel Research Institute |
引用本文:
张北江; 赵光普; 胥国华; 冯涤 . GH742合金热变形行为与微观组织演化[J]. 金属学报, 2005, 41(11): 1207-1214 .
,
,
,
.
Hot deformation behavior and micro-structure evolution of superalloy GH742[J]. Acta Metall Sin, 2005, 41(11): 1207-1214 .
[1] Long Z D, Zhuang J Y, Deng B, Zhong Z Y. Acta Metall Sin, 1999; 35: 1211 (龙正东,庄景云,邓波,仲增墉.金属学报,1999;35:1211) [2] Meyers M A, Benson D J, Vohringer O, Kad B K, Xue Q,Fu H H. Mater Sci Eng, 2002; A322: 194 [3] Semiatin S L, Weaver D S, Fagin P N, Glavicic M G. Metall Mater Trans, 2004; 35A: 679 [4] Hayes R W. Acta Metall, 1983; 31: 365 [5] Doherty R D, Hughes D A, Humphreys F J, Jonas J J.Mater Sci Eng, 1997; A238: 219 [6] Prasad Y, Seshacharyulu T. Int Mater Rev, 1998; 43: 243 [7] Shen G S, Semiatin S L, Shivpuri R. Metall Mater Trans,1995; 26A: 1795 [8] Verdier M, Brechet Y, Guyot P. Acta Mater, 1999; 47:127 [9] Sakai T, Ohashi M, Jonas J J. Acta Metall, 1988; 36: 1781 [10] Verdier M, Brechet Y, Guyot P. Acta Mater, 1999; 47:127 [11] Speer J G, Hasen S S. Metall Trans, 1989; 20A: 25 [12] Simmons J P, Wen Y, Shen C, Wang Y Z. Mater Sci Eng,2004; A365: 136 [13] Gourdet S, Montheillet F. Acta Mater, 2003; 51: 2685 [14] Song X Y, Markus R, Zhang J X. Acta Metall Sin, 2004; 40: 1009 (宋晓艳,Markus R,张久兴.金属学报,2004;40:1009) [15] McQueen H J, Ryan N D. Mater Sci Eng, 2002; A322: 43 [16] Weertman J. J Appl Phys, 1957; 28: 362 [17] Bruni C, Forcellese A, Gabrielli F. Mater Sci Technol,2002; 125: 242 [18] Siddall R J, Eggar J W. Mater Sci Technol, 1986; 2: 728 [19] Wahabi M E, Cabrera J M, Prado J M. Mater Sci Eng,2003; A343: 116 [20] Briottet L, Jonas J J, Monthellet F. Acta Mater, 1996;44:1665 [21] Gottstein G, Kocts U. Acta Metall, 1983; 31: 175 [22] Sakai T, Jonas J J. Acta Metall, 1984; 32: 189 [23] Crespo D, Pradell T, Clavaguera N. Mater Sci Eng, 1997;A238: 160 [24] Kazaryan A, Wang Y, Dregia S A, Patton B R. Acta Mater, 2002; 50: 2491 [25] Tian B, Wang Y, Zickler G A, Lind C, Paris O. Acta Mater, 2003; 51: 4149 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|