					引用本文:
						|  |  
    					|  |  
    					| 超高强度块体Al90Mn8Ce2合金 |  
						| 赵占奎  姚可夫  李建忱 蒋 青 |  
					| 清华大学机械工程系; 北京 100084 |  
						|  |  
    					| BULK Al90Mn8Ce2 ALLOY WITH ULTRA HIGH STRENGTH |  
						| ZHAO Zhankui; YAO Kefu; LI Jianchen; JIANG Qing |  
						| Department of Mechanical Engineering; Tsinghua University; Beijing 100084 |  
								赵占奎; 姚可夫; 李建忱; 蒋青                                                                                                                                                                                                                                      . 超高强度块体Al90Mn8Ce2合金[J]. 金属学报, 2004, 40(4): 355-358       .	
																												,
																								 ,
																								 ,
																												 . 
				BULK Al90Mn8Ce2 ALLOY WITH ULTRA HIGH STRENGTH[J]. Acta Metall Sin, 2004, 40(4): 355-358       .
 
					
						| 
								
									|  
          
          
            
                         
            
									            
									                
																														  
																| [1] Cahn R W. Nature, 1989; 341: 183 [2] Inoue A. Prog Mater Sci, 1998; 43: 365
 [3] Wang J Q, Tseng M K, Hao Y Y, Hu Z Q, Wang Z G.Mater Sci Eng, 1998; A247: 51
 [4] Kim Y H, Inoue A. Mater Trans JIM, 1990; 31: 747
 [5] Kawamura Y, Mano H, Inoue A. Scr Mater, 2001; 44:1599
 [6] Schurack F, Eckert J, Schultz L. Ada Mater, 2001; 49:1351
 [7] Zhao Z K, Li J C, Jiang Q. Mater Sci Technol, 2002; 18:1241
 [8] Ye F, Lu K. Acta Mater, 1999; 47: 2449
 [9] Dash J G. Rev Mod Phys, 1999; 71: 1737Y
 |  
             
												
											    	