双相材料中相间内应力的X射线测量与表征 |
姜传海 程凡雄 吴建生 |
上海交通大学材料科学与工程学院高温材料及高温测试教育部重点实验室; 上海 200030 |
|
MEASUREMENT AND REPRESENTATION OF THE INTER--PHASE STRESS FOR DOUBLE-PHASE MATERIAL BY X-RAY METHOD |
JIANG Chuanhai; CHENG Fanxiong; WU Jiansheng |
Key Laboratory for High Temperature Materials and Tests of Ministry of Education; School of Materials Science and Engineering; Shanghai Jiaotong University; Shanghai 200030 |
引用本文:
姜传海; 程凡雄; 吴建生 . 双相材料中相间内应力的X射线测量与表征[J]. 金属学报, 2004, 40(4): 351-354 .
,
,
.
MEASUREMENT AND REPRESENTATION OF THE INTER--PHASE STRESS FOR DOUBLE-PHASE MATERIAL BY X-RAY METHOD[J]. Acta Metall Sin, 2004, 40(4): 351-354 .
[1] Noyan I C, Cohen J B. Residual Stress Measurement by Diffraction and Interpretation, Springer-Verlag Press, 1989: 54 [2] Zhang D Q, He J W. Residual Stress Analysis by X-ray Diffraction and Its Functions, Xi'an: Xi'an Jiaotong University Press, 1999: 3(张定铨,何家文.残余应力的X射线分析与作用,西安:西安 交通大学出版社, 1999:3) [3] Ledbetter H M, Austin M W. Mater Sci Eng, 1987; 89:53 [4] Sun Z M, Li J B, Wang Z G, Li W J. Acta Metall Mater,1992; 40(11) : 2961 [5] Sun Z M, Li J B, Wang Z G, Lu S X. Physical Testing andChemical Analysis Part A, Physical Testing, 1992; 28(2) ;38(孙正明,李家宝,王中光,吕毓雄.理化检验物理分册. 1992;28(2) :38) [6] Taya M, Arsenault R J. Metal Matrix Composites Ther-moraechanical Behavior. Pergamon Press, 1989: 23 [7] Jiang C H, Wang D Z, Yao Z K. Acta Metall Sin, 2000; 36: 555(姜传海,王德尊,姚忠凯.金属学报, 2000;36:555) [8] Jiang C H, Wang D Z, Yao C K, J Mater Sci Lett, 1999;18: 901 [9] Yang Y X, Qi X. Analysis by X-ray Diffraction, Shanghai:Shanghai Jiaotong University Press, 1994: 140(杨于兴,漆 玄. X射线衍射分析,上海:上海交通大学出版社, 1994:140) |
|