| Mn含量对低碳钢中铁素体动态再结晶的影响 |
| 李龙飞;杨王玥;孙祖庆 |
| 北京科技大学材料科学与工程学院; 北京 100083 |
|
| INFLUENCE OF Mn CONTENT ON DYNAMIC RECRYSTALLIZATION OF FERRITE IN LOW CARBON STEELS |
| LI Longfei; YANG Wangyue;SUN Zuqing |
| School of Materials Science & Engineering; University of Science & Technology Beijing; Beijing 100083 |
引用本文:
李龙飞; 杨王玥; 孙祖庆 . Mn含量对低碳钢中铁素体动态再结晶的影响[J]. 金属学报, 2004, 40(12): 1257-1263 .
,
,
.
INFLUENCE OF Mn CONTENT ON DYNAMIC RECRYSTALLIZATION OF FERRITE IN LOW CARBON STEELS[J]. Acta Metall Sin, 2004, 40(12): 1257-1263 .
[1] Zhou R F,Yang W Y, Sun Z Q. Acta Metall Sin, 2004; 40:1 (周荣锋,杨王玥,孙祖庆.金属学报,2004;40:1) [2] Glover G, Sellars C M. Metall Trans, 1973; 4: 765 [3] Tsuji N, Matsubara Y, Saito Y. Scr Mater, 1997; 37: 477 [4] Najafi-Zadeh A, Jonas J J, Yue S. Metall Trans, 1992;23A: 2607 [5] Gao F, Xu Y, Song B, Xia K. Metall Trans, 2000; 31A:21 [6] Yagi H, Tsuji N, Saito Y. Tetsu Hagane, 2000; 86: 349 [7] Li L F, Yang W Y, Sun Z Q. Acta Metall Sin, 2003; 39:419 (李龙飞,杨王玥,孙祖庆.金属学报,2003;39:419) [8] Yang W Y, Wang H M, Li L F, Sun Z Q. Acta Metall Sin,2003; 39: 691 (杨王玥,王红梅,李龙飞,孙祖庆.金属学报,2003;39:691) [9] Li L F, Yang W Y, Sun Z Q. Acta Metall Sin, 2004; 40:141 (李龙飞,杨王玥,孙祖庆.金属学报,2004;40:141) [10] Kohsaku U, Naoki Y, Osamu A, ISIJ Int, 1994; 34: 85 |
|