|
|
|
| 高温度梯度下Al-In偏晶合金定向凝固组织的演化规律 |
| 崔红保;郭景杰;毕维生;苏彦庆;吴士平;傅恒志 |
| 哈尔滨工业大学材料科学与工程学院; 哈尔滨 150001 |
|
| THE EVOLUTION OF UNIDIRECTIONAL SOLIDIFI-CATION MICROSTRUCTURE OF THE Al-In MONOTECTIC ALLOYS IN HIGH TEMPERATURE GRADIENT |
| CUI Hongbao; GUO Jingjie; BI Weisheng; SU Yanqing; WU Shiping; FU Hengzhi |
| Department of Materials Science and Engineering; Harbin Institute of Technology; Harbin 150001 |
引用本文:
崔红保; 郭景杰; 毕维生; 苏彦庆; 吴士平; 傅恒志 . 高温度梯度下Al-In偏晶合金定向凝固组织的演化规律[J]. 金属学报, 2004, 40(12): 1253-1256 .
,
,
,
,
,
.
THE EVOLUTION OF UNIDIRECTIONAL SOLIDIFI-CATION MICROSTRUCTURE OF THE Al-In MONOTECTIC ALLOYS IN HIGH TEMPERATURE GRADIENT[J]. Acta Metall Sin, 2004, 40(12): 1253-1256 .
[1] Xie H, Wang J C, Fan J F, Hao W X, Yang G C. Hot Work Technol, 2003; (4): 49 (谢辉,王锦程,樊建锋,郝维新,杨根仓.热加工工艺,2003; (4):49) [2] Liu Y, Guo J J, Jia J. Foundry, 2000; 49(1):1 (刘源,郭景杰,贾均.铸造,2000;49(1):1) [3] Xian A P, Zhang X M, Li Z Y, Liu Q Q, Chen J Z, Li Y Y. Acta Metall Sin, 1996; 32: 113 (冼爱平,张修睦,李忠玉,刘清泉,陈继志,李依依.金属学 报, 1996;32:113) [4] Hayes L J, Andrews J B. Mater Sci Forum, 2000; 329-330:209 [5] Stoker C, Ratke L. J Cryst Growth, 2000; 212: 324 [6] Stoker G, Ratke L. J Cryst Growth, 1999; 203: 582 [7] Aoi I, Makoto I, Yoshida M, Fukunagab H, Nakaea H. JCryst Growth, 2001; 222: 806 [8] Grugel N G, Lograsso T A. Metall Trans, 1984; 15A:1003 [9] Cai Y W, Li J G. Chin J Mater Res, 1995; 9; 208 (蔡英文,李建国.材料研究学报,1995;9:208) [10] Kamio A, Kumai S, Tezuka H. Mater Sci Eng, 1991; A146:105 [11] Zhang D L, Cantor B. Acta Metall Mater, 1991; 39: 1595 [12] Arikawa Y, Andrews J B, Coriell S R, Mitchell W F. In: Schiffman R A, Andrews J B, eds., 6th Int Symp on Experimental Methods for Microgravity Materials Science, at the 123rd Annual TMS Meeting, Warrendale, PA: TMS Minerals, Metals & Materials Society, 1994: 110 [13] Chadwick G A. Br J Appl Phys, 1965; 16: 1095 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|