| 长期高温时效F12耐热合金钢中碳化物形态和组分变化 |
| 胡正飞; 杨振国 |
| 复旦大学材料科学系; 上海 200433 |
|
| The Morphological and Compositional Changes of the Carbides in F12 Heat-Resistant Alloy Steel for Long-Term Service at Elevated Temperature |
| HU Zhengfei; YANG Zhenguo |
| Department of Science Materials; Fudan University; Shanghai 200433 |
引用本文:
胡正飞; 杨振国 . 长期高温时效F12耐热合金钢中碳化物形态和组分变化[J]. 金属学报, 2003, 39(2): 131-135 .
,
.
The Morphological and Compositional Changes of the Carbides in F12 Heat-Resistant Alloy Steel for Long-Term Service at Elevated Temperature[J]. Acta Metall Sin, 2003, 39(2): 131-135 .
[1] Bendick W, Harrmann K, Wellnitz G, Zschau M. VGBKraftwerkstech, 1993; 73: 73 [2] Coutsouradis D. Proc COST 501/OEC Cof, Dordrecht:Kluwer Academic Publications, 1994: 1 [3] Germany Standard, DIN17175, Nahtlose Rohre ausWarmfesten Stahken-Techniscche Lieferbedingungen,1979 [4] Beffzzieche P. MM VGB, 1958; 57: 393 [5] Hu Z F, Wu X F, Wang C X. Ada Metall Sin, 2001; 37:381(胡正飞,吴杏芳,王春旭.金属学报, 2001;37:381) [6] Hahn B, Bendick W. VGB Kraftwerkstechnik, 2000; 11: 85 [7] Battaini P, Dangelo D, Marino G, Hald J. In: Wilshire B, Evans R W eds., Proc 4th Int Conf on Creep and Fracture of Engineering Materials and Structures, London: The Institute of Metals, 1999: 1039 [8] Klimanek P, Cyrener K, Germain C, Jenkner K, Martin U, Oettel O, Ostwaldt A, Ostwaldt D, Pantleon W. In: Mughrabi H ed., Micro structures and Mechanical Properties of Metallic High-Temperature Materials. Bonn: Deutsche Forschungsgemeinschaft, 1999: 272 [9] Kuo K H (Guo K X), Ye H Q, Wu Y K. Application of Electron Diffraction Patterns in Orystallgraph. Beijing: Science Press, 1983: 426(郭可信,叶恒强,吴玉琨.电子衍射图在晶体学中的应用,北京:科学出版社,1983:426) [10] Zschau M, Niederhoff K. VGB Kraftwerkstech, 1994; 74:111 [11] Lundin L, Andren H O. Micron Microsc Acta, 1991; 22:159 [12] Strang A, Vodarek V. In: Strang A ed., Microstructure ofHigh Temperature Materials. No.2. London: The Institute of Metal, 1998: 117 [13] Vodarek V, Strang A. Scr Mater, 1998; 38: 101 [14] Eggeler G. Acta Metall, 1989; 37: 3225 [15] Thomson R C, Bhadeshia H K D H. Metall Trans, 1992;23A: 1171 [16] Cahn R W, Haasen P. Phys Metall. Part Ⅱ , Netherlands:North-Holland Physics Publishing, 1983: 1541 [17] Kruszynska J S, Piekarski K R, Taplin D M R. Mater SciTechnol, 1985; 1: 118 |
|