| 304不锈钢非比例循环棘轮行为的实验研究 |
| 康国政 高庆 |
| 西南交通大学应用力学与工程系; 成都 610031 |
|
引用本文:
康国政; 高庆 . 304不锈钢非比例循环棘轮行为的实验研究[J]. 金属学报, 2000, 36(5): 497-501 .
[1] Chaboche J L, Nouailhas D. ASME J Eng Mater Technol,1989; 111: 384 [2] Hassan T, Kyriakides S. Int J Plast, 1992; 8: 91 [3] Hassan T, Kyriakides S. Int J Plast,1994;10:149 [4] Yang X J, Gao Q, Cai L X. Acta Aeronaut Astronaut Sin,1997; 18(4): 395(杨显杰,高 庆,蔡力勋.航空学报,1997;18(4:395) [5] Yang X J, Kang G Z, Gao Q, Sun Y F. Acta Metall Sin,1999; 35(7): 698(杨显杰,康国政,高 庆,孙亚芳.金属学报,1999; 35(7):698) [6] Jiang Y, Sehitoglu H. Int J Plast, 1994; 10: 579 [7] McDowell D L. Int J Plast, 1995; 11: 397 [8] Yoshida F. Eur J Mech A/Solids, 1995; 14(1): 97 |
|