|
|
|
| Cr6Mn13Ni10/Cr5Mo异质接并没有时效过程中碳的扩散行为 |
| 王立刚 王来 黄明亮 董贵昕 王富岗 |
| 大连理工大学材料工程系;大连 116024 |
|
引用本文:
王立刚; 王来; 黄明亮; 董贵昕; 王富岗 . Cr6Mn13Ni10/Cr5Mo异质接并没有时效过程中碳的扩散行为[J]. 金属学报, 1999, 35(8): 883-887 .
[1] Huang M L. Thesis of Master's Degree, Dalian University of Technology, 1995 (黄明亮硕士学位论文,大连理工大学,1995) [2] Huang M L, Wang L Metall Trans , 1999; A29: 3037 [3] Lundin C D Weld Res, 1982;(Suppl ): 58 [4] Lei Y B,Xin Y B,Li P N,Ge X X ,Xhang J Q Press Vesel 1992 9:379 (雷月葆,忻云彪,李培宁,葛修鑫,张金权压力容器,1992;9: 379) [5] Pavlovsky J, Million B, Ciha K, Stransky K· Mater Sci Eng 1991 A149:105 [6] He K S, Cao X F. Welding of Dissimilar Metal Beijing: Mechanical Industry Press, 1986: 85 何康生,曹雄夫 异种金属焊接 北京:机械工业出版社,1986: 85) [7] Wang L,Huang M L J Dalian Univ Technol, 1999 39 77王来,黄明亮 大连理工大学学报,1999;39:77) [8] Dong G X . Thesis of Master's Degree, Dalian University of Technology, 1997 (董贵昕 硕士学位论文,大连理工大学,1997) [9] Cheng B L. Principle of Welding Metallurgy. Beijing: Qin hua Uiversity Press,199且:261 (陈伯螫.焊接冶金原理北京:清华大学出版社,1991:261) [10] Zhou Z F. Principle and Process of Metal Welding(Second), Beijing:Mechanism Industry Press,1981:228 周振丰.金属熔焊原理及工艺(下册)北京:机械工业出版社, 1981:228) |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|