| A1—Cu合金凝固过程中准固态力学性能及微量元素的影响 |
| 魏晓伟;曾明;吴学婷 |
| 四川工业学院材料科学与工程系;成都;611744;四川工业学院材料科学与工程系;成都;611744;四川工业学院材料科学与工程系;成都;611744 |
|
| MECHANICAL PROPERTIES OF QUASI-SOLID Al-Cu ALLOY AND INFLUENCE OF TRACE ELEMENTS DUING SOLIDIFICAfION |
| WEI Xiaowei; ZENG Ming; WU Xueting(Department of Materials Science and Engineering; Sichuan Institute of Industry; Chengdu 611744) |
引用本文:
魏晓伟;曾明;吴学婷. A1—Cu合金凝固过程中准固态力学性能及微量元素的影响[J]. 金属学报, 1998, 34(7): 719-724.
,
,
.
MECHANICAL PROPERTIES OF QUASI-SOLID Al-Cu ALLOY AND INFLUENCE OF TRACE ELEMENTS DUING SOLIDIFICAfION[J]. Acta Metall Sin, 1998, 34(7): 719-724.
1 Chijiiwa K, Nishda K. J Fac Eng Univ Tokyo, 1976; B4: 38 2 Tamman G, Rooha Z. Z Metallk, 1933, 24: 131 3 Singer A R E, Cottrell S A. J Inst Met, 1947; 73: 33 4H 1966: 166(Novikov E E. The Red Brittleness of Nonferrous Metal and Alloy. Moscow: The State Machinery ManufactureBook Press, 1966: 166) 5千千岩健儿,林守仁铸物,1981;53:161(Chijiiwa K; Hnyashi M. IMONO, 1981; 53: 161) 6矶部俊夫,久保田昌男,北岗山治铸物,19782 50:235(Isobe T, Kubota M, Kitaoka S IMONO, 1978; 50: 235) 7矶部俊夫,久保田昌男,北岗山治铸物,1978;50:425(Isobe T, Kubota M, Kitaofor S. IMONO, 1978 50: 425) 8矶部俊夫,久保田昌男,北岗山治铸物,1981; 53: 153(Isobe T, Kubota M; Kitaoka S. IMONO, 1981 53: 153) 9林清 ,中日毅铸物,1982;54:599 (Lin Ching-Tsan, Nakata T IMONO, 1982; 54: 599) 10李庆春,周彼德,曾松岩金属科学与工艺,1983;2(3):66(LI Qingchun,Zhou Bide,Zeng Songyan.Met Sci Technol,1983; 2(3):66) 11刘驰,陈魁英,李庆春材料科学与工艺,1993;1(1):64(Liu Chi ,Chen Kuiying,Li Qingchun.Mater Sci Technol,1993;1(1):64) 12刘驰,李庆春,曾松岩材料科学进展,1989;3:447(Liu Chi,Li Qingchun,Zeng Songyan.Mater Sci Progr,1989; 3:447) 13贾宝仟,柳百成特种铸造及有色合金,1997;(2):4(Jia Baoqian,Liu Baicheng.Spec Cast Nonferrous Alloys,1997(2):4) 14胡汉起金属凝固北京:冶金工业出版社,1985:151(Hu Hanqi. Solidification of Metals.Beijing:The Metallurgical Industry Press,1985:151) 15雄谷重夫,户田善久,大矢泰正铸物,1979; 51:533(Ora S, Toda Z, Ora Y. IMONO, 1979; 51: 533) 16朱培铀,陈玉勇,李庆春铸造,1984;(1):25(Zhu Peiyue, Chen Yuyong, Li Qingchun. Foundry, 1984;(1): 25) 17Kissling R J, Wallace J F. Foundry,1963;(7): 45 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|