| SiC_p增强铝基复合板材力学性能与晶粒取向分布 |
| 陈礼清;吕毓雄;毕敬 |
| 中国科学院金属研究所;沈阳;110015;中国科学院金属研究所;沈阳;110015;中国科学院金属研究所;沈阳;110015 |
|
| MECHANICAL PROPERTIES AND CRYSTALLITE ORIENTATION DISTRIBUTION OF SiC_p REINFORCED ALUMINIUM MATRIX COMPOSITE SHEETS |
| CHEN Liqing;L U Yuxiong;BI Jing (Institute of Metal Research;Chinese Academy of Sciences;Shenyang 110015) |
引用本文:
陈礼清;吕毓雄;毕敬. SiC_p增强铝基复合板材力学性能与晶粒取向分布[J]. 金属学报, 1998, 34(11): 1183-1187.
,
,
.
MECHANICAL PROPERTIES AND CRYSTALLITE ORIENTATION DISTRIBUTION OF SiC_p REINFORCED ALUMINIUM MATRIX COMPOSITE SHEETS[J]. Acta Metall Sin, 1998, 34(11): 1183-1187.
1Dayvidson D L.Metall Trans,1991;22A:113 2Llovd D J. Int Mater Rev, 1994; 39: 1 3 Beck Tan N C, Aikin Jr R M, Briber R M. Metall Materl Trans, 1994: 25A:2461 4 Felli F,Brotzu A.DiRusso E,Pinna F. Mater Sol Technol,1997:13:420 5 Singh P M,Lewandowski J J. Metall Trans,1993:24A:2531 6Doel T J A. Bowen P Mater Set Eng, 1996; 12:586 7 DoelT J A, Loretto M H,Bowen P Composites,1993;24:270 8 Wang B,Janowski G M,Patterson B R.Metall Mater Trans,1995;26A:2457 9 Liang Z D, Xu J Z,Wang F In:Nagashima S ed;Proc of 6th Int Coof on Textures of Materials.Tokyo, ISIJ, 1986:2:1259 10 Arsenault R J,Shi N.Mater Sci Eng,1986; 81:175 11 Nardone V C,Prewo K M. Scr Metall, 1986; 20: 43 12 Lee C S,Duggan B J, Metall Trans.1991;22A:2637 13 Choi C H,Kwon J W, Oh K H,Lee D N.Acta Mater,1997:45:511 |
|