| 焊接热循环对HQ130钢热影响区组织及性能的影响 |
| 李亚江;邹增大;陈祝年;魏星;江全昌 |
| 山东工业大学;厦门工程机械股份有限公司 |
|
| EFFECTS OF THE WELD THERMAL CYCLE ON MICROSTRUCTURE AND PROPERTIES OF THE HEAT-AFFECTED ZONE OF HQ130 STEEL |
| LI Yajiang;ZOU Zengda;CHEN Zhunian;WEI Hing(Shandong Polytechnic University; Jinan 250014); JIANG Quanchang(Engineering Machinery Co. Ltd. Xiamen361004)(Manuscript received 1995-10-04) |
引用本文:
李亚江;邹增大;陈祝年;魏星;江全昌. 焊接热循环对HQ130钢热影响区组织及性能的影响[J]. 金属学报, 1996, 32(5): 532-537.
,
,
,
,
.
EFFECTS OF THE WELD THERMAL CYCLE ON MICROSTRUCTURE AND PROPERTIES OF THE HEAT-AFFECTED ZONE OF HQ130 STEEL[J]. Acta Metall Sin, 1996, 32(5): 532-537.
| 1罗志昌,姚钦,田燕,张伟民,郎毅,侯丽.焊接学报,1990;11(3):1692尹士科,王移山.钢铁研究学报,1991;1:653HassonDF,ZanisCA,AndersonDR.MeldJ,1984;63(6):1974FraserFW,MetzbowerEA.WeldJ,1982;61(4):1125ChenC,ThomponAW,BernsteinIM.MetallTrans,1980;11A:1723 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|