Please wait a minute...
金属学报  1996, Vol. 32 Issue (5): 538-543    
  论文 本期目录 | 过刊浏览 |
Ni-Fe-Cr-B-Si涂层超塑扩散焊接的强化效应及耐磨性
李延祥;文九巴;祝要民;黄金亮
洛阳工学院;西安交通大学
STRENGTHENING AND WEAR RESISTANCE OF Ni-Fe-Cr-B-Si SPRAY ALLOY COATING BY SUPERPLASTICAL DIFFUSION WELDING
LI Yanxiang;WEN Jiuba;ZHU Yaomin(Luoyang Institute of Technology; Luoyang471039); HUANG Jinliang (Xi'an Jiaotong University; Xi'an 710049)(Manuscript received 1995-07-11)
引用本文:

李延祥;文九巴;祝要民;黄金亮. Ni-Fe-Cr-B-Si涂层超塑扩散焊接的强化效应及耐磨性[J]. 金属学报, 1996, 32(5): 538-543.
, , , . STRENGTHENING AND WEAR RESISTANCE OF Ni-Fe-Cr-B-Si SPRAY ALLOY COATING BY SUPERPLASTICAL DIFFUSION WELDING[J]. Acta Metall Sin, 1996, 32(5): 538-543.

全文: PDF(450 KB)  
摘要: 研究了Ni-Fe-Cr-B-Si合金涂层超塑性扩散焊接及焊接后的强化效应。通过对涂层的组织结构分析、硬度及耐磨性能的测试表明,当基材(5CrMnMo钢)与涂层产生协调超塑变形时,涂层原颗粒间、涂层与基材结合界面完全焊合。超塑焊合后的涂层比高频重熔及火焰重熔涂层硬度(HV)提高100-150,耐摩擦磨损性能提高30%。指出,沉淀强化、细晶强化及晶内位错密度增加是引起涂层强化效应和提高耐磨性的主要因素。
关键词 : Ni-Fe-Cr-B-Si合金涂层,  超塑性扩散焊接,  强化效应    
Abstract:The structural analysis and tests of hardness and wear resistance of Ni-Fe-Cr-B-Si coating indicated that the original coating particles and the interfaces between coating and substrate were readily jointed if the substrate of 5CrMnMo steel together with coating deformed superplastically. The hardness of the superplastical diffusion welded coating may be superior to that of high frequency induction or spray remelted coatings up to 100-150%, and wear resistance up to 30%. It is seemed that the major factors of the improvement of the strengthening and wear resistance of the coating welded may be precipiation hardening, fine grained structure and increasing in internal dislocation density.
Key words: Ni-Fe-Cr-B-Si alloy coating    superplastical diffusion welding    strengthening
收稿日期: 1996-05-18     
基金资助:河南省自然科学基金
1AC著,刘春林译.金属与合金的超塑效应.北京:科学技术出版社,1983:542PillingJ,LiveseyDW,HawkyardJB,RidleyN.MetSci,1984;3:1173李延祥,文九巴,黄金亮,祝要民.金属学报,1994;30:B1364TangS著,宋玉泉,齐安民译.超塑性力学,长沙:湖南大学出版社,1989:365高彩桥.摩擦金属学.哈尔滨:哈尔滨工业大学出版社,1988:141-186
[1] 张贵锋; 张建勋; 张华; 裴怡; 王士元 . 预置中间层的相变超塑性焊接新工艺及其接头组织[J]. 金属学报, 2003, 39(6): 655-660 .
[2] 刘平; 康布熙; 曹兴国; 黄金亮; 顾海澄 . 快速凝固Cu-Cr合金时效析出的共格强化效应[J]. 金属学报, 1999, 35(6): 561-564 .