第三元素对TiAl基双相合金组织的影响 |
谢英秀;曹名洲;徐曾基 |
中国科学院金属研究所;中国科学院金属研究所十室;副研究员;沈阳110015;中国科学院金属研究所 |
|
EFFECT OF THIRD ALLOYING ELEMENTS ON DOUBLE-PHASE STRUCTURE OF TiAI BASE ALLOYS |
XIE Yingxiu;CAO Mingzhou;XU Zengji Institute of Metal Research; Academia Sinica; Shenyang associate professor;Institute of Metal Research;Academia Sinica; Shenyang 110015 |
引用本文:
谢英秀;曹名洲;徐曾基. 第三元素对TiAl基双相合金组织的影响[J]. 金属学报, 1993, 29(4): 13-18.
,
,
.
EFFECT OF THIRD ALLOYING ELEMENTS ON DOUBLE-PHASE STRUCTURE OF TiAI BASE ALLOYS[J]. Acta Metall Sin, 1993, 29(4): 13-18.