Ti对高Al-Zn合金组织性能的影响 |
刘金水;舒震;李传平 |
湖南大学机械工程系;副教授;长沙410082;湖南大学;长沙410082;湖南大学;长沙410082 |
|
INFLUENCE OF TI ON STRUCTURE AND PROPERTLES OF HIGH Al-Zn ALLOYS |
LIU Jinshui;SHU Zhen;LI Chuanping Hunan University; Changsha |
引用本文:
刘金水;舒震;李传平. Ti对高Al-Zn合金组织性能的影响[J]. 金属学报, 1993, 29(11): 9-13.
,
,
.
INFLUENCE OF TI ON STRUCTURE AND PROPERTLES OF HIGH Al-Zn ALLOYS[J]. Acta Metall Sin, 1993, 29(11): 9-13.
1 Hadbiby F, Mcnallan M J. Trans Am Foundrymen's Soc, 1984; 92: 263 2 舒震,刘金水.湖南大学学报,1988;2:42 3 骆灼旋,陈华信.铸造,1992;4:28 4 Shu Zhen, Liu Jinshui. Proceedings of Shenyang International Symposium on Casting. 1988; 445 5 Apellian D, Paliwal M. J Met, 1981; 11: 12 6 Pearson W B. A Handbook of Lattice Spacing and Structures of Metals and Alloys. Oxford: Pergamon, 1958: 363e |
|