| 微量Mg在M2高速钢中的作用 |
| 毛卫民;钟雪友 |
| 北京工业大学金属材料系;讲师;北京100022;北京科技大学 |
|
| BEHAVIOUR OF TRACE Mg IN HIGH SPEED STEEL M2 |
| MAO Weimin Beijing Polytechnic University University of Science and Technology Beijing |
引用本文:
毛卫民;钟雪友. 微量Mg在M2高速钢中的作用[J]. 金属学报, 1993, 29(11): 14-17.
,
.
BEHAVIOUR OF TRACE Mg IN HIGH SPEED STEEL M2[J]. Acta Metall Sin, 1993, 29(11): 14-17.
1 Sandberg H. Scandi J of Metall, 1973; 2: 233 2 Gierek A, Marciak A, Wusatowski R. Zesz Nauk Politech Slask. 1982; 23: 5 3 #12 4 #12 5 Ghomashchi M R,Sellars C M. Met Sci, 1984; 18: 44 6 Holye G, Ineson E. Jpn Iron Steel Inst, 1959; 193: 254 7 #12 8 Lenta E J,Pesci H,Twentyman M E. Metallography, 1983; 16: 387 9 Fredriksson H, Hillert M, Nica M. Scand J Metall, 1979; 8: 115 |
|