| 球铁中奥氏体枝晶对力学性能的影响 |
| 周继扬;谢祖华;钟凤琪 |
| 大连理工大学;大连理工大学;大连理工大学 |
|
| INFLUENCE OF AUSTENITIC DENDRITES ON MECHANICAL PROPERTIES OF DUCTILE IRON |
| ZHOU Jiyang;XIE Zuhua;ZHONG Fengqi Dalian University of Technology |
引用本文:
周继扬;谢祖华;钟凤琪. 球铁中奥氏体枝晶对力学性能的影响[J]. 金属学报, 1992, 28(3): 92-94.
,
,
.
INFLUENCE OF AUSTENITIC DENDRITES ON MECHANICAL PROPERTIES OF DUCTILE IRON[J]. Acta Metall Sin, 1992, 28(3): 92-94.
1 周继扬,谢祖华,钟凤琪.铸造,1991;(3) :9--14 2 Gagne M, Goller R. Trans Am Foundrymen's Soc, 1983; 91: 37--46 3 Barton R. Giesserei, 1978; 65: 294--301{ |
|