| Nb对(Nd,Dy)-(Fe,Co)-B永磁体显微组织的影响 |
| 宋晓平;王笑天;黄启华;刘军海;姚引良 |
| 西安交通大学;讲师;西安交通大学;西安交通大学;西安交通大学;西安交通大学 |
|
| EFFECT OF Nb ADDITION ON MICROSTRUCTURE OF (Nd,Dy)-(Fe,Co)-B MAGNETS |
| SONG Xiaoping;WANG Xiaotian;HUANG Qihua;LIU Junhai;YAO Yinliang Xi'an Jiaotong University |
引用本文:
宋晓平;王笑天;黄启华;刘军海;姚引良. Nb对(Nd,Dy)-(Fe,Co)-B永磁体显微组织的影响[J]. 金属学报, 1991, 27(5): 120-124.
,
,
,
,
.
EFFECT OF Nb ADDITION ON MICROSTRUCTURE OF (Nd,Dy)-(Fe,Co)-B MAGNETS[J]. Acta Metall Sin, 1991, 27(5): 120-124.
1 Kim A S. J Appl Phys, 1988; 63: 3975 2 Xiao Y, Strnat K J, Mildrum H F, Ray A E. In: Herget C, Poerschke R eds., Proc 9th Int Workshop on Rare Earth Magnets and their Applications and 5th Int Symposium on Magnetic Anisotropy and Coercivity in Rare Earth-Transition Metal Alloys, Vol.Ⅰ, 31, Aug. 3 Sep., 1987, Bad Soden, FRG, Bad Honnef 1, FRG: DPG-GmbH, 1987: 467 3 Tokunaga M., Kogure H, Endoh M, Harada H IEEE Trans Magn, 1987; 23: 2287 4 Rodewald W, Wall B. J Magn Magn Mater, 1989; 80: 57 5 Parker S F H, Grundy P J, Fidler J. J Magn Magn Mater, 1987; 66: 74 6 Ishikawa T, Hamada Y, Ohmort K. IEEE Trans Magn, 1989; 25: 3434 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|