| 铸造/热压Pr-Fe-B磁体的矫顽力及其与晶粒尺寸关系 |
| 陈钟敏;谢发勤;史正兴;王乐仪;傅恒志 |
| 西北工业大学;讲师现在西安交通大学材料系;西北工业大学;西北工业大学;西北工业大学;西北工业大学 |
|
| COERCIVITY AND ITS GRAIN SIZE DEPENDENCE IN CAST-HOT PRESSED Pr-Fe-B MAGNETS |
| CHEN Zhongmin;XIE Faqin;SHI Zhengxing;WANG Leyi;FU Hengzhi Northwestern Polytechnical University; Xi'an |
引用本文:
陈钟敏;谢发勤;史正兴;王乐仪;傅恒志. 铸造/热压Pr-Fe-B磁体的矫顽力及其与晶粒尺寸关系[J]. 金属学报, 1991, 27(5): 125-129.
,
,
,
,
.
COERCIVITY AND ITS GRAIN SIZE DEPENDENCE IN CAST-HOT PRESSED Pr-Fe-B MAGNETS[J]. Acta Metall Sin, 1991, 27(5): 125-129.
1 Livingston J D. J Appl Phys, 1981; 52: 2544 2 陈钟敏,谢发勤,史正兴,王乐仪,傅恒志.中国稀土学报,1990;8:281 3 Sagawa M, Hirosawa S. J Mater Res, 1988: 3: 45 4 Brown W F Jr. J Appl Phys, 1962; 33: 3022 5 McIntyre D A. J Phys D: Applied Physics, 1970; 3: 1430 6 Ramesh R, Srikrishna K. J Appl Phys, 1988; 64: 6406 7 Ramesh R, Thomas G, Ma B M. J Appl Phys. 1988; 64: 6416 8 罗阳,张宁,苏秀锦.金属学报,1987;23;A136 |
|