| MnCu合金马氏体相变和马氏体的内耗 |
| 王力田;葛庭燧 |
| 中国科学院固体物理研究所;沈阳;中国科学院固体物理研究所 |
|
| 0412-1961 |
| INTERNAL FRICTION IN MARTENSITE AND MARTENSITIC TRANSFORMATION IN MnCu ALLOYS |
引用本文:
王力田;葛庭燧. MnCu合金马氏体相变和马氏体的内耗[J]. 金属学报, 1988, 24(3): 147-154.
,
.
0412-1961[J]. Acta Metall Sin, 1988, 24(3): 147-154.
1 Bacon G E, Dummur I W, Smith I H, Street R. Proc. R. Soc. London. A. 1957: 241: 223 2 冯端,王业宁,丘第荣.金属物理,下册,科学出版社,1975:611 3 Sugimoto K, Mori T, Shiode S. Met Sci J, 1973; 7: 103 4 文亦汀,王力田,杜家驹.物理,1986;15(2) :109 5 Smith I H, Vance E R. J Appl Phys, 1969; 40: 4853 6 Nowick A S, Berry B S. Anelastic Relaxation in Crystalline Solids, New York: Academic Press 1972: 9 |
|