高性能再生硬质合金的短流程回收制备* |
王瑶, 刘雪梅, 宋晓艳(), 魏崇斌 王海滨, 王西龙 |
北京工业大学材料科学与工程学院新型功能材料教育部重点实验室, 北京100124 |
|
SHORT-TERM PROCESS OF RECYCLING CEMENTED CARBIDE SCRAPS AND PREPARATION OF HIGH PERFORMANCE HARD METALS |
WANG Yao, LIU Xuemei, SONG Xiaoyan(), WEI Chongbin, WANG Haibin, WANG Xilong |
Key Laboratory of Advanced Functional Materials, College of Materials Science and Engineering, Beijing University of Technology, Beijing 100124 |
引用本文:
王瑶, 刘雪梅, 宋晓艳, 魏崇斌 王海滨, 王西龙. 高性能再生硬质合金的短流程回收制备*[J]. 金属学报, 2014, 50(5): 633-640.
Yao WANG,
Xuemei LIU,
Xiaoyan SONG,
Chongbin WEI,
Haibin WANG,
Xilong WANG.
SHORT-TERM PROCESS OF RECYCLING CEMENTED CARBIDE SCRAPS AND PREPARATION OF HIGH PERFORMANCE HARD METALS[J]. Acta Metall Sin, 2014, 50(5): 633-640.
[1] |
Fag Z Z, Wang X, Ryu T, Hwang K S, Sohn H Y. Int J Refract Met Hard Mater, 2009; 27: 288
|
[2] |
Wei C B, Song X Y, Fu J, Liu X M, Wang H B, Gao Y, Wang Y. Cryst Eng Comm, 2013; 15: 3305
|
[3] |
Liu S, Yi D Q, Li Y X, Zou D. Acta Metall Sin (Engl Lett), 2002; 15: 448
|
[4] |
Kim H C, Shon I J, Yooh J K, Doh J M. Int J Refract Met Hard Mater, 2007; 25: 46
|
[5] |
Xiong Y H, Lau K, Zhou X Y, Schoenung J M. J Clean Prod, 2008; 16: 1118
|
[6] |
Venkateswaran S, Schubert W D, Lux B. Int J Refract Met Hard Mater, 1996; 14: 263
|
[7] |
Zhang Q X, Zhang J X. Rare Met Cem Carbides, 1995; (4): 48
|
[7] |
(张齐勋, 张家雄. 稀有金属与硬质合金, 1995; (4): 48)
|
[8] |
Lee J C, Kim E Y, Kim J H, Kim W, Kim B S, Pandey B D. Int J Refract Met Hard Mater, 2011; 29: 365
|
[9] |
Hu Y J, Sun P M, Li H G, Chen A L. Rare Met Cem Carbides, 2004; 32(3): 53
|
[9] |
(胡宇杰, 孙培梅, 李洪桂, 陈爱良. 稀有金属与硬质合金, 2004; 32(3): 53)
|
[10] |
Sun B Q. Rare Met Cem Carbides, 1998; (3):12
|
[10] |
(孙宝琦. 稀有金属与硬质合金, 1998; (3): 12)
|
[11] |
Liu W B, Song X Y, Zhang J X, Zhang G Z, Liu X M. Int J Refract Met Hard Mater, 2009; 27: 115
|
[12] |
Zhang W B, Sha C S, Du Y, Wen G H, Xie W, Wang S Q. Acta Metall Sin, 2011; 47: 1307
|
[12] |
(张伟彬, 沙春生, 杜 勇, 温光华, 谢 文, 王社权. 金属学报, 2011; 47: 1307)
|
[13] |
Cao Z M, Song X Y, Qiao Z Y. Rare Met, 2008; 32: 216
|
[13] |
(曹战民, 宋晓艳, 乔芝郁. 稀有金属, 2008; 32: 216)
|
[14] |
Wei C B, Song X Y, Fu J, Lv X S, Wang H B, Gao Y, Zhao S X, Liu X M. J Mater Sci Technol, 2012; 28: 837
|
[15] |
Zhao S X, Song X Y, Liu X M, Wei C B, Wang H B, Gao Y. Acta Metall Sin, 2011; 47: 1188
|
[15] |
(赵世贤, 宋晓艳, 刘雪梅, 魏崇斌, 王海滨, 高 杨. 金属学报, 2011; 47: 1188)
|
[16] |
Joost R, Pirso J, Viljus M, Letunovits S, Juhani K. Est J Eng, 2012; 18: 127
|
[17] |
Liu W B, Song X Y, Zhang J X, Zhang G Z, Liu X M. Mater Chem Phy, 2008; 109: 235
|
[18] |
Konyashin I, Hlawatschek S, Ries B, Lachmann F, Dorn F, Sologubenko A, Weirich T. Int J Refract Met Hard Mater, 2009; 27: 234
|
[19] |
Christensen M, Wahnström G. Phys Rev, 2003; 67B: 115415
|
[20] |
Jia K, Fischer T E, Gallois B. Nanostruct Mater, 1998; 10: 875
|
[21] |
Fang Z Z. Int J Refract Met Hard Mater, 2005; 23: 119
|
[22] |
Fang Z Z, Lockwood G, Griffo A. Metall Mater Trans, 1999; 30A: 3231
|
[23] |
Wang X, Hwang K S, Koopman M, Fang Z Z, Zhang L H. Int J Refract Met Hard Mater, 2013; 36: 46
|
[24] |
Song S H, Li J C. Acta Metall Sin, 1987; 23: 521
|
[24] |
(宋士泓, 李健纯. 金属学报, 1987; 23: 521)
|
[25] |
Liu M L, Huang X Y, Duan S T, Shao D Q, Cui Y M, Yao Z M. Acta Metall Sin, 1982; 18: 689
|
[25] |
(刘曼朗, 黄孝瑛, 段石田, 邵大琴, 崔玉梅, 姚振梅. 金属学报, 1982; 18: 689)
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|