静水压力对超纯Al/超纯Fe电偶中超纯Al腐蚀行为的影响 |
马荣耀1,2,穆鑫1,刘博3,王长罡1,魏欣1,赵林1,董俊华1( ),柯伟1 |
1. 中国科学院金属研究所 沈阳 110016 2. 中国科学院大学 北京 100049 3. 东北大学冶金学院 沈阳 110819 |
|
Effect of Hydrostatic Pressure on Corrosion Behavior of Ultra Pure Al Coupled with Ultra Pure Fe |
MA Rongyao1,2,MU Xin1,LIU Bo3,WANG Changgang1,WEI Xin1,ZHAO Lin1,DONG Junhua1( ),KE Wei1 |
1. Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China 2. University of Chinese Academy of Sciences, Beijing 100049, China 3. School of Metallurgy, Northeastern University, Shenyang 110819, China |
引用本文:
马荣耀, 穆鑫, 刘博, 王长罡, 魏欣, 赵林, 董俊华, 柯伟. 静水压力对超纯Al/超纯Fe电偶中超纯Al腐蚀行为的影响[J]. 金属学报, 2019, 55(12): 1593-1605.
MA Rongyao,
MU Xin,
LIU Bo,
WANG Changgang,
WEI Xin,
ZHAO Lin,
DONG Junhua,
KE Wei.
Effect of Hydrostatic Pressure on Corrosion Behavior of Ultra Pure Al Coupled with Ultra Pure Fe[J]. Acta Metall Sin, 2019, 55(12): 1593-1605.
[1] | Ma R Y, Zhao L, Wang C G, et al. Influence of hydrostatic pressure on the thermodynamics and kinetics of metal corrosion [J]. Acta Metall. Sin., 2019, 55: 281 | [1] | (马荣耀, 赵 林, 王长罡等. 静水压力对金属腐蚀热力学及动力学的影响 [J]. 金属学报, 2019, 55: 281) | [2] | Xing S H, Li Y, Wharton J A, et al. Effect of dissolved oxygen and coupled resistance on the galvanic corrosion of Cr-Ni low-alloy steel/90-10 cupronickel under simulated deep sea condition [J]. Mater. Corros., 2017, 68: 1123 | [3] | Li Q C, Yang J, Wu L, et al. Influence of pressure on galvanic corrosion of 907/921/B10 couples in simulated deep-sea environment [J]. Int. J. Electrochem. Sci., 2016, 11: 6443 | [4] | Mansfeld F, Chen C, Lee C C, et al. The effect of asymmetric electrodes on the analysis of electrochemical impedance and noise data [J]. Corros. Sci., 1996, 38: 497 | [5] | Lowe A M, Eren H, Bailey S I. Electrochemical noise analysis: Detection of electrode asymmetry [J]. Corros. Sci., 2003, 45: 941 | [6] | Chen J F, Bogaerts W F. Electrochemical emission spectroscopy for monitoring uniform and localized corrosion [J]. Corrosion, 1996, 52: 753 | [7] | Bertocci U, Gabrielli C, Huet F, et al. Noise resistance applied to corrosion measurements: I. Theoretical analysis [J]. J. Electrochem. Soc., 1997, 144: 31 | [8] | Bertocci U, Huet F. Noise resistance applied to corrosion measurements: III. Influence of the instrumental noise on the measurements [J]. J. Electrochem. Soc., 1997, 144: 2786 | [9] | Bautista A, Huet F. Noise resistance applied to corrosion measurements: IV. Asymmetric coated electrodes [J]. J. Electrochem. Soc., 1999, 146: 1730 | [10] | Bautista A, Bertocci U, Huet F. Noise resistance applied to corrosion measurements: V. Influence of electrode asymmetry [J]. J. Electrochem. Soc., 2001, 148: B412 | [11] | Cottis R A. The significance of electrochemical noise measurements on asymmetric electrodes [J]. Electrochim. Acta, 2007, 52: 7585 | [12] | Curioni M, Cottis R A, Di Natale M, et al. Corrosion of dissimilar alloys: Electrochemical noise [J]. Electrochim. Acta, 2011, 56: 6318 | [13] | Curioni M, Cottis R A, Di Natale M, et al. Electrochemical noise analysis on multiple dissimilar electrodes: Theoretical analysis [J]. Electrochim. Acta, 2011, 56: 10270 | [14] | Curioni M, Balaskas A C, Thompson G E. An alternative to the use of a zero resistance ammeter for electrochemical noise measurement: Theoretical analysis, experimental validation and evaluation of electrode asymmetry [J]. Corros. Sci., 2013, 77: 281 | [15] | Curioni M, Cottis R A, Thompson G E. Interpretation of electrochemical noise generated by multiple electrodes [J]. Corrosion, 2013, 69: 158 | [16] | Curioni M, Skeldon P, Thompson G E. Reliability of the estimation of polarization resistance of corroding electrodes by electrochemical noise analysis: Effects of electrode asymmetry [J]. Electrochim. Acta, 2013, 105: 642 | [17] | Astarita A, Curioni M, Squillace A, et al. Corrosion behaviour of stainless steel-titanium alloy linear friction welded joints: Galvanic coupling [J]. Mater. Corros., 2015, 66: 111 | [18] | Blasco-Tamarit E, Igual-Mu?oz A, García Antón J, et al. Corrosion behaviour and galvanic coupling of titanium and welded titanium in LiBr solutions [J]. Corros. Sci., 2007, 49: 1000 | [19] | Sakairi M, Shimoyama Y, Takahashi H. Electrochemical noise analysis of galvanic corrosion of anodized aluminum in chloride environments [J]. Electrochemistry, 2006, 74: 458 | [20] | Sakairi M, Shimoyama Y. Electrochemical random signal analysis during galvanic corrosion of anodized aluminum alloy [J]. J. JSEM, 2007, 7(Spec. issue):114 | [21] | Monta?és M T, Sánchez-Tovar R, García-Antón J, et al. Influence of the flowing conditions on the galvanic corrosion of the copper/AISI 304 pair in lithium bromide using a zero-resistance ammeter [J]. Int. J. Electrochem. Sci., 2010, 5: 1934 | [22] | Sun H J, Liu L, Li Y, et al. The performance of Al-Zn-In-Mg-Ti sacrificial anode in simulated deep water environment [J]. Corros. Sci., 2013, 77: 77 | [23] | Gusmano G, Montesperelli G, Pacetti S, et al. Electrochemical noise resistance as a tool for corrosion rate prediction [J]. Corrosion, 1997, 53: 860 | [24] | Cottis R A. Interpretation of electrochemical noise data [J]. Corrosion, 2001, 57: 265 | [25] | Ma R Y, Wang C G, Mu X, et al. Influence of hydrostatic pressure on corrosion behavior of ultrapure Fe [J]. Acta Metall. Sin., 2019, 55: 859 | [25] | (马荣耀, 王长罡, 穆 鑫等. 静水压力对超纯Fe腐蚀行为的影响 [J]. 金属学报, 2019, 55: 859) | [26] | Rilling G, Flandrin P, Goncalves P. On empirical mode decomposition and its algorithms [A]. Proceedings of the IEEE-EURASIP Workshop on Nonlinear Signal and Image Processing [C]. Grado, Italy: IEEE, 2003: 8 | [27] | Flandrin P, Rilling G, Goncalves P. Empirical mode decomposition as a filter bank [J]. IEEE Signal Process. Lett., 2004, 11: 112 | [28] | Cao C N. Principles of Electrochemistry of Corrosion [M]. Beijing: Chemical Industry Press, 2008: 105 | [28] | (曹楚南. 腐蚀电化学原理 [M]. 北京: 化学工业出版社, 2008: 105) | [29] | Shao Y W, Huang H, Zhang T, et al. Corrosion protection of Mg-5Li alloy with epoxy coatings containing polyaniline [J]. Corros. Sci., 2009, 51: 2906 | [30] | Cao F H, Zhang Z, Su J X, et al. Electrochemical noise analysis of LY12-T3 in EXCO solution by discrete wavelet transform technique [J]. Electrochim. Acta, 2006, 51: 1359 | [31] | Aballe A, Bethencourt M, Botana F J, et al. Wavelet transform-based analysis for electrochemical noise [J]. Electrochem. Commun., 1999, 1: 266 | [32] | Dong Z H, Guo X P, Zheng J S, et al. Calculation of noise resistance by use of the discrete wavelets transform [J]. Electrochem. Commun., 2001, 3: 561 | [33] | Moshrefi R, Mahjani M G, Jafarian M. Application of wavelet entropy in analysis of electrochemical noise for corrosion type identification [J]. Electrochem. Commun., 2014, 48: 49 | [34] | Aballe A, Bethencourt M, Botana F J, et al. Using wavelets transform in the analysis of electrochemical noise data [J]. Electrochim. Acta, 1999, 44: 4805 | [35] | Cai C, Zhang Z, Cao F H, et al. Analysis of pitting corrosion behavior of pure Al in sodium chloride solution with the wavelet technique [J]. J. Electroanal. Chem., 2005, 578: 143 | [36] | Homborg A M, van Westing E P M, Tinga T, et al. Novel time-frequency characterization of electrochemical noise data in corrosion studies using Hilbert spectra [J]. Corros. Sci., 2013, 66: 97 | [37] | Homborg A M, Tinga T, Zhang X, et al. Transient analysis through Hilbert spectra of electrochemical noise signals for the identification of localized corrosion of stainless steel [J]. Electrochim. Acta, 2013, 104: 84 | [38] | Zhao B, Li J H, Hu R G, et al. Study on the corrosion behavior of reinforcing steel in cement mortar by electrochemical noise measurements [J]. Electrochim. Acta, 2007, 52: 3976 |
|
|